Friday, March 4, 2016

Re: [MW:24431] Re: How to protect Serration of Flanges during Hot dip galvanization

Hi

Request Client to accept or re machine it with the manufacturer or machine shops.

No chemical is available to clean, since the serrated surfaces might have fused.

With kind regards
Govindan

On 11 Feb 2016 07:00, "Hamid Jabbari" <lifebod@gmail.com> wrote:
Does any one know how could i remove the hot galvanized coating from face of flange?
plz advise


On Monday, August 23, 2010 at 1:08:56 PM UTC+4:30, aly mhaskar wrote:


Dear All,
Presently we are doing hot dip galvanization of pipe spools where we have to protect the serration of flanges during galvanization.
 
Can any body suggest what can be applied on serration to protect it from adhesion of ZINC on serration.
 
Thank you in advance.
 
Mhaskar Aly
Kuwait




--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/75d1da68-c97b-4709-b526-afb7cfd25136%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CANiuf9fDXK15j02%3DaVNy7Zug3JChTso4vgpgir9g0qOiY8e4zg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...