Dear Friend,

As per API 650, Cls 7.5 it was mention in dimension tolerance topic
that The bulging of bottom plate shall not exceed .25% of dia of tank
(for tank dia <40m) unless otherwise mentioned. 100mm max. for tank
dia >40m.


Thanks,
Bala
On 2/22/16, Vishal Sharma <vishalsharma.sharma225@gmail.com> wrote:
> Dear Experts,
>
> We found 42 mm distortion in bottom plate after welding with shell. Is it
> acceptable? Please share reference standard.
> Please note tank fabrication is going on within shop.
>
> Br,
> Vishal Sharma
>
> --
> You received this message because you are subscribed to the Google Groups
> "Materials & Welding" group.
> To unsubscribe from this group and stop receiving emails from it, send an
> email to materials-welding+unsubscribe@googlegroups.com.
> To post to this group, send email to materials-welding@googlegroups.com.
> Visit this group at https://groups.google.com/group/materials-welding.
> To view this discussion on the web visit
> https://groups.google.com/d/msgid/materials-welding/CAAK1segupjbGRtScdgV3DhDP4k-7sx2y_NjnfcBC8fovg-g6ag%40mail.gmail.com.
> For more options, visit https://groups.google.com/d/optout.
>

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAL9C6DZrbSwc5tMi682DccWMTykG_nbBOi25vgxUFvscyJM5VA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...