Hi,
Plan for a WPS & PQR – it will resolve all your issues…
And plan for a Demo to for the speed of operation.
Thanks & Regards,
Lakshman Kumar B,
+91 9440031459.
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Dinesh Somwanshi
Sent: Tuesday, March 08, 2016 2:35 PM
To: materials-welding
Subject: [MW:24446] Welding process selection.
Dear sir,
I need 1 help from you that as following.
1. we are doing bridge fabrication for L & T as per indian standard.For fillet stiffener welding they have approved SMAW .
During SMAW we found numer of undercuts & slow process in welding.
2. We have recommended to use FCAW E71T-C welding process instead of SMAW E7018 . They are partially agreed & asking to submit that process comparison to choose FCAW to ensure that it fullfill the strenght of weld.
Please share your opinion.
DINESH VITTHAL SOMWANSHI
BACHELOR IN MECHANICAL ENGINEER
AUTHORIZED WELDING / NDT / PAINTING INSPECTION PERSONNEL,
AWS - CWI , CSWIP 3.1
BGAS Gr 2 / 3
NDT II -UT , RT , MT , PT, VT
00919881344135
असो द्यावी दया तुमच्या लागतसे पाया.
Pray for others, sometime, You might never need to pray for yourself again.....
--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAELgRrV5ynQAB-jEQ3Jq4mFfb5ccQJXgkTZytBW6hFLuR%3DBvBA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
No comments:
Post a Comment