[MW:14166] Change in Manufacturer for Plate Requires MPQT in Line pipe

Dear Experts,
 
         One of the Manufacturer initially rolled the line pipe (API 5L) for the line item x ( dia 44" x 16.9 mm) with Voset Alpine plates, for the same manufacturer conducted Manufacturer Procedure Qualification test (MPQT) and the result found satisfactory. As there was not enough quantity of plates to complete the line item Manufacturer informed the line item x will be rolled after procuring the plates. Mean time manufacturer rolled for other line items of the same P.O with different sizes. Manufacturer received the plates from Sumitomo instead of Voest alpine to complete the partially rolled line item x ( dia 44" x 16.9 mm). In this case whether manufacturer shall conduct MPQT once again for the Sumitomo Plates for the line item x ( dia 44" x 16.9 mm) or elsae we shall conduct test unit only instead of MPQT. Please clear my doubt.

--
G.Murali krishnan

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Comments

Punit Dubey said…
Dear Murali

MPQT should be carried out with the change of manufacturing process of line pipe.
As supplier is changing the steel source/steel making and rolling practice (and hence the manufacturing process of steel which is a part of line pipe manufacturing process), hence MPQT should be repeated.
Also have a close look over line pipe specification you may also find some details over there.

Regards

Punit Dubey
9925150566

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...

The Schaeffler and Delong diagrams for predicting ferrite levels in austenitic stainless steel welds

Introduction Ferrite is important in avoiding hot cracking in during cooling from welding of austenitic stainless steels. 'Constitution diagrams' are used to predict ferrite levels from the composition by comparing the effects of austenite and ferrite stabilising elements. The Schaeffler and Delong diagrams are the original methods of predicting the phase balances in austenitic stainless steel welds. Nickel and chromium equivalents A 'nickel equivalent' is calculated for the austenite stabilising elements and a 'chromium equivalent' ferrite stabilising elements. These are used as the axes for the diagrams, which show the compositional equivalent areas where the phases austenite, ferrite, martensite (and mixtures of these) should be present. Although intended to show the phase balance of weld fillers, these diagrams can also be used to illustrate the phase balance of the 'parent' material. There are different diagrams for dif...