Skip to main content

Re: [MW:14075] Impact test report of PTC

Dear Shadab, salam
 
We have welded PTC with qualified wps with E70S2 @ minus 48deg C,
 
Test was carried out for weld,
 
Ali
 
 
-------Original Message-------
 
Date: 05/04/2012 09:44:27
Subject: Re: [MW:14064] Impact test report of PTC
 

Dear Ali,
The consumable for tig Filler metal ER70S2 is not suitable for impact test @-48 degrees.
Also want to know the heat input and location of charpy impact test.

Regards
Shadab

On Apr 5, 2012 7:50 AM, "Aly" <mhaskar.aly@gmail.com> wrote:
Low temp vessel PTC for head to shell c-seam; Head : Cap SA420WPL6, Pipe: SA333 Gr 6; Filler metal ER70S2+ E7018-1; GTAW+ SMAW process.
 
PTC used as filler metal is not SFA classified for low temp -48deg C
 
Impact test results: 18, 14, 12 Joules test piece size 10 x 7.5 x 55 @ -48deg C;
 
Average value required for 10x 7,5x55 is 15joule; single specimen 2/3 x 15: 10joule
 
Reference ASME SEC VIII Div-1 2011a UG 84 & UCS 67
 
Dear Expert,
Let me have your advice whether these results are acceptable.
 
Thanks
Aly
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...