Skip to main content

RE: [MW:12536] spot radiography as per ASME B 31.3

Dear Azhar

 

Your version “Spot Radiography is to be taken on joint but random examination is be selected from the lot”

 

I have the following comments :-

 

01.  In all cases the Radiography is always on the weld joints only

02.  Random is always from the different weld seams of a vessel

 

But the basic question is not yet replied.

 

May be Experts can shed some more light on this matter

 

Best regards

 

 

Nachhattar Singh,

Tel: +91 98201 81158 / +91 22 27580036

Email: nsingh@librainspection.com

            

407/408, Vindhya Commercial Complex,

Sector 11, CBD Belapur

Navi Mumbai - 400 614

Maharashtra, India.

www.librainspection.com

 

PLEASE THINK BEFORE PRINTING

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Azam Mohd
Sent: Monday, September 26, 2011 12:12 PM
To: materials-welding@googlegroups.com
Subject: Re: [MW:12533] spot radiography as per ASME B 31.3

 

Dear Azhar,

Spot Radiography is to be taken on joint but random examination is be selected from the lot.

 

Thanks & Regards,

Mohd.Azam

On Mon, Sep 26, 2011 at 8:47 AM, Azhar Ali <aab51214@yahoo.com> wrote:

DEAR EXPERTS

 

let me know the extent of radiography as per ASME B31.3 for normal service.

 

Can any body elaborate the the difference between spot and random examination as per para no.344.1.3. 

 

 

Regards

 

Azhar Ali

 

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...