Skip to main content

[MW:12500] RE: 12497] Query regarding use of CS Fasteners and CS Blind Flanges for Hydrotest of SS Vessel

Dear Friend,

 

You are almost correct - that blind flange and bolts should be of the same material as vessel material,

But if nothing is specified in drawing means it may not be that much particular about the material for client.

So you may also proceed for CS Bolts and Dummy,

However it’s better to take client view also to make the drawings correct, and to choose 100%suitable material.

 

 

Thanks and Regards................?

 

Lakshman Kumar.B|Manager- QA/QC |Lanco Infratech Limited

Plot No 1255 | Sanjeevani chowk | Mahanadi vihar | Cuttack 753004

Phone : + 91 671 2445033 | Mobile : +91 9937286851 |www.lancogroup.com

Go Green|The future will thank you

 

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of asad azmi
Sent: Wednesday, September 21, 2011 6:49 PM
To: materials-welding@googlegroups.com
Subject: [MW:12497] Query regarding use of CS Fasteners and CS Blind Flanges for Hydrotest of SS Vessel

 

 Dear ALL,

 

Greetings.


Please refer below Client Specfication which quotes  ---
  
Hydrostatic pressure testing shall be performed with gaskets and bolting identical to those required in service and as specified on the data sheet. These gaskets may be used as service gaskets if the bolted joint is not disassembled after completion of hydrostatic pressure testing.
 
I believe as per the above requirment only SS Fasteners and Blind flanges shall be used during the hydrotest  of
 SS Vessel UNLESS Data Sheet/Drawing is allowing to use CS Fasteners and Blind flanges for hydrotest.
 
Please suggest.
 
Thanks & Regards
 
Asad Azmi
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...