Skip to main content

RE: [MW:12581] Tension Test Requirement for SA 283 Gr.C plates

You have to identify heat number and lot number of all these plates, and then decide number of tests.

 

BR

 

HWCai

Sulzer

 


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Pieper QSI
Sent: Thursday, September 29, 2011 12:40 AM
To: materials-welding@googlegroups.com
Subject: RE: [MW:12575] Tension Test Requirement for SA 283 Gr.C plates

 

It seems to me that when every plate has similar heat and plate number they will be produced from a coil, especially when the thickness is 6 mm.

 

Met vriendelijke groeten / Best Regards

 

Herman Pieper

 

Pieper Quality Support & Inspection

Phone: +31 (0)521 380083

Fax:     +31 (0)84 7539225

Cell:     +31 (0)6 51691215

www.pieper-qsi.nl

 

Van: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] Namens asad azmi
Verzonden: woensdag 28 september 2011 16:29
Aan: materials-welding@googlegroups.com
Onderwerp: Re: [MW:12573] Tension Test Requirement for SA 283 Gr.C plates

 

SA 20 is not applicable here.



 

On Wed, Sep 28, 2011 at 2:10 PM, Bathula Raghuram (Mumbai - PIPING) <R.Bathula@ticb.com> wrote:

One tension test coupon shall be taken from each plate-as-rolled (para 11.1.1 of SA20).

 

Note: plate-as-rolled— the quantity of plate product rolled at one time, either from an individual slab or directly from an ingot.

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of asad azmi
Sent: Wednesday, September 28, 2011 3:59 PM
To: materials-welding@googlegroups.com
Subject: [MW:12567] Tension Test Requirement for SA 283 Gr.C plates

 

Dear All,

 

Greetings.

 

 

As per MTC for the plates material - SA283GR C,  for a single Heat number( 10K22884)  total 15 Nos of plates are supplied having plate no. 15942 

 

Description of Goods- Hot rolled steel plates with sheared edges. Plates are in Non Heatreated  condition.

 

MTC is showing only  2 tension test results.

 

Please clarify whether only two tension test are acceptable OR there shall be 15 nos of tension test for 15 plates.( 1 tension test for each plate)

 

Thanks & Regards

 

Asad Azmi


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

CONFIDENTIALITY NOTICE
The information in this email may be confidential and/or privileged.
This email is intended to be reviewed by only the addressee(s) named
above. If you are not the intended recipient, you are hereby notified
that any review, dissemination, copying, use or storage of this email
and its attachments, if any, or the information contained herein is
prohibited. If you have received this email in error, please
immediately notify the sender by return email and delete this email
from your system. Thank you.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...