Re: [MW:12537] spot radiography as per ASME B 31.3



Dear Sir,
This is as per 2004 edition. 

341.5.1 Spot Radiography
(a) Longitudinal Welds. Spot radiography for longitudinal groove welds required to have a weld joint factor
Ej of 0.90 requires examination by radiography in accordance with para. 344.5 of at least 300 mm (1 ft) in each
30 m (100 ft) of weld for each welder or welding operator.
Acceptance criteria are those stated in Table 341.3.2 for
radiography under Normal Fluid Service.
(b) Circumferential Butt Welds and Other Welds. It is
recommended that the extent of examination be not less
than one shot on one in each 20 welds for each welder
or welding operator. Unless otherwise specified, acceptance criteria are as stated in Table 341.3.2 for radiography under Normal Fluid Service for the type of joint
examined.
(c) Progressive Sampling for Examination. The provisions of para. 341.3.4 are applicable.
(d) Welds to Be Examined. The locations of welds and
the points at which they are to be examined by spot



Thanking You,

Honesty is the best Policy

With Warm Regards,

Muthu Barathi P
Mobile No:00962788269821 (Jordan)
00962775401951


From: "Nachhattar Singh" <nsingh@librainspection.com>
Sent: Mon, 26 Sep 2011 13:36:56
To: <materials-welding@googlegroups.com>
Subject: Re: [MW:12536] spot radiography as per ASME B 31.3

Dear Azhar

 

Your version "Spot Radiography is to be taken on joint but random examination is be selected from the lot"

 

I have the following comments :-

 

01.  In all cases the Radiography is always on the weld joints only

02.  Random is always from the different weld seams of a vessel

 

But the basic question is not yet replied.

 

May be Experts can shed some more light on this matter

 

Best regards

 

 

Nachhattar Singh,

Logo-Libra-Version12

Tel: +91 98201 81158 / +91 22 27580036

Email: nsingh@librainspection.com

            

407/408, Vindhya Commercial Complex,

Sector 11, CBD Belapur

Navi Mumbai - 400 614

Maharashtra, India.

www.librainspection.com

 

PLEASE THINK BEFORE PRINTING

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Azam Mohd
Sent: Monday, September 26, 2011 12:12 PM
To: materials-welding@googlegroups.com
Subject: Re: [MW:12533] spot radiography as per ASME B 31.3

 

Dear Azhar,

Spot Radiography is to be taken on joint but random examination is be selected from the lot.

 

Thanks & Regards,

Mohd.Azam

On Mon, Sep 26, 2011 at 8:47 AM, Azhar Ali <aab51214@yahoo.com> wrote:

DEAR EXPERTS

 

let me know the extent of radiography as per ASME B31.3 for normal service.

 

Can any body elaborate the the difference between spot and random examination as per para no.344.1.3. 

 

 

Regards

 

Azhar Ali

 

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


Follow Rediff Deal ho jaye! to get exciting offers in your city everyday.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...