Re: [MW:12509] Requirement of No. of Thermocouples.

Mr.Vichare,
The no. of thermocouple for PWHT, it is no written any where in the code but ones the procedure is approved, it should be follwed. if you whant change the no of thermocouple you can reverse the procedure. But normaly what is the client requirment that should be follwed, like thermocuople type and distence between thermocouple, heating & cooling rate, Unrestricted heating & cooling rate and etc.... I have seen that diffrent procedure one is requried up to 2" 1thermocouple, 2" to 4" two and 6" to 18" three and more ......
other one procedure up to 8" one, 8" to 24" two and etc....
 
Regards
Jesti


--- On Fri, 9/23/11, Ramchandra vichare <vicharerke@indiatimes.com> wrote:

From: Ramchandra vichare <vicharerke@indiatimes.com>
Subject: [MW:12507] Requirement of No. of Thermocouples.
To: materials-welding@googlegroups.com
Date: Friday, September 23, 2011, 12:09 AM

Dear Experts,

With reference to the above mentioned subject , during Heat-treatment of Piping spool joints I insisit one of my vendor to used thermocouples as noted below:-
Up to 4"NB = 1 no.(Bottom side)
Above 4" to 8"NB= 2 nos.(top & Bottom)(say 180Deg.)
8" to 24"= 3 nos (120Deg)
Above 24" =4 nos.
and according to accepted Heattreatment Procedure it was alo acceptable but unfortunitaly delay in Heat treat the joint; vendor is not ready to follow Procedure due to the reseason referred above & no where written in ASME 31.3 regarding the requirement of Tharmocouples.  Reauested experts to Guide guaide me why we are placing thromocouples? I think it is control soaking anyhow;let me tell  were I will get ready reference and documentryevidence for requiremnt of Number of thermocouples? Is any effect during soaking time or any metallourgicval changes will be there if we use one thermocouple instead of above? . Pl be guaide in detail with documentry evidence.


Regards,

RK Vichare
Mumbai-India

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...