Skip to main content

[MW:988] Re: 985] Re: HAZ

Dear Mr Mahuri
Please post your querries with appropriate subject line and also don't
club different querries together

Thanking for your cooperation

On Jul 31, 5:50 pm, "Mahuri Snehkumar \(TIPO - QA/QC\)"
<S.Mah...@panipat.ticb.com> wrote:
> Dear Bose,
>
> The difference what you have mentioned that I am also well aware of, but I require some other major difference.
>
> Regards,
>
> Snehkumar L. Mahuri
> Lead - Welding / NDE
> EPCC 2A, PANIPAT
> 9215989508
>
> -----Original Message-----
> From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Rituraj Bose
> Sent: Thursday, July 31, 2008 3:32 PM
> To: Materials & Welding
> Subject: [MW:985] Re: HAZ
>
> Dear Mahuri,
>
> Actually length of HAZ cannot be specified so easily. In any case you
> can follow the link to have just an idea for it.
>
> http://www.esabna.com/us/en/education/knowledge/qa/How-does-welding-a...
>
> Regarding your 2nd question I can tell that the Code name itself
> identifiy the difference.
> API 650 is for the "Welded Steel Tanks for Oil Storage" and API 620 is
> for the "Design and Construction of Large, Welded, Low-Pressure
> Storage Tanks".
>
> Regards,
>
> R. Bose
>
> On Jul 29, 7:11 am, "Mahuri Snehkumar \(TIPO - QA/QC\)"
> <S.Mah...@panipat.ticb.com> wrote:
> > Dear friends,
>
> > Can someone tell me the exact length of HAZ area after the weld.
>
> > Also what is the main difference between API 650 and API 620 codes.
>
> > Regards,
>
> > Snehkumar L. Mahuri
>
> > Lead - Welding / NDE
>
> > EPCC 2A, PANIPAT
>
> > 9215989508
>
> > image001.gif
> > 92KViewDownload
--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

Comments

Anonymous said…
very useful read. I would love to follow you on twitter.

Popular posts from this blog

Re: [MW:34105] SA266 GR4N 4 Cycle SPWHT

Hi,  You are correct, Minimum refers to the one cycle for which this part will expose until final work shop PWHT. hence mill test certificate shall include this.  Max. SPWHT, refers to additional cycles of heat treatment that are reserved for future repairs during equipment lifetime.  Again, these simulated no. Of cycles shall be specified in MTC.  The idea is we need to make sure that steel mechanical properties are not compromised upon exposure to multiple repairs (i e 4 cycles in your case).  One could say, if steel is subjected to 4 cycles and is ok, then it should by defacto be good for one cycle, yet, this is wrong assumption cause mechanical problems and microstructure of materials varies accordingly based on no. Of cycles for which material will expose. This is apparent in alloy steel and especially for impact test values as an example.  In your case, this forged CS with properties before PWHT can be understood to be " as forged" condition (i.e. Wit...

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...