Skip to main content

[MW:912] RE: 880] clarification reg root gap

Keep 2.5 mm to 3.2 mm root gap.

-----Original Message-----
From: materials-welding@googlegroups.com
[mailto:materials-welding@googlegroups.com] On Behalf Of Bathula Anil
Kumar
Sent: 22 June, 2008 1:47 AM
To: materials-welding@googlegroups.com
Subject: [MW:880] clarification reg root gap

Dear Friends,

My Name is Anil Kumar working as a Quality Control Inspector in Qatar,
for Decon for an Oil Refinery project. I Joined the company recently and
during my regular visits to site and also reviewing various data sheets
I found that most of the defects are Root undercut, LOP and LOF, the
welding used for the production is TIG welding with 2.4mm filler wires
for all SS, CS and LTCS materials the Dia of the pipes ranges from 2inch
to 24 inch and yeah there is lot of problem with the material reg the
mismatch and ovality in the pipe apart from this another prob I observe
that the root gap used for the welding is mostly 4+ mm for all the
joints , I strongly recommended for 2.5 to 3.5 mm at the max for the
Root gap but some of the welders complaining that they are finding
difficulty in moving the electrode.

I request you to kindly suggest me what is the root gap for the above
said materials and what are the other possibilities for the above said
repairs and the corrective action required to be taken for the same.

I thank you one and all very much for creating such a beautiful group

Thanking you,

Regards

Bathula Anil Kumar

Visakhapatnam


________________________________

From Chandigarh to Chennai - find friends all over India. Click here.
<http://in.rd.yahoo.com/tagline_groups_10/*http://in.promos..yahoo.com/g
roups/citygroups/>

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...