[MW:950] RE: 948] Re: why CC2235-9 is not applicable for ASME Sec.III

In my opinion neither code nor CC distinguishes the diff. between flaw direction longitudinal/transverse (please correct me I am a level zero in UT), hence your interpretation could be correct.

However Fig2 of CC shows something transverse and longitudinal planar flaws (could we interpret like that?)

 


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of raghavendra pemmaraju
Sent: Saturday, July 19, 2008 7:52 PM
To: materials-welding@googlegroups.com
Subject: [MW:948] Re: why CC2235-9 is not applicable for ASME Sec.III

 

Dear All,

One more query, this time related to acceptance criteria as per ASME CodeCase 2235-9.

For the flaws oriented transverse to weld centre line axis, what is the acceptance criteria as per above CC.

As per me the above CC is silent on this and hence we need to apply the same acceptance criteria as mentioned in tables 1,2 &3 of above CC. What is your opinion.!!!!

 

regards,

Raghavendra

 
--- On Wed, 7/16/08, raghavendra pemmaraju <pemma_raghav@yahoo.com> wrote:

From: raghavendra pemmaraju <pemma_raghav@yahoo.com>
Subject: [MW:931] why CC2235-9 is not applicable for ASME Sec.III
To: materials-welding@googlegroups.com
Date: Wednesday, July 16, 2008, 10:28 PM

We are aware that ASME code case 2235-9 is appliabcle for ASME Sec.I,Sec.VIII and Sec.XII. Why not the same is applicable incase of ASME Sec.III. Where as if we see the philosophy of the above CodeCase is mainly drawn from the nuclear code ASME Sec.XI at the same time.

Can any one comment on the above.

 

regards,

Raghavendra

ASNT Level III ( RT,UT & MT) & RSO L-III

Manager,QC

L&T Ltd., Hazira

Surat

 



 


--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Re: [MW:14950] RE: 14919] Stress relieving Rejected for 5 min less soaking time.

Dear All, I have been a CONSULTANT FOR such problem & my personal opinion is expressed as follow. I fully agree with views expressed so far. But bag to differ that " Code is a law, with engineering judgments. Hence the inspector has the rights to declare that the original HT was inadequate." Inspectors & total industry must resist the "REJECTION" . We as intellectual & having seniority must become practical. How the code will revise???. ANS.: One is experiments (Pure research) & second is such chances that gives opportunity to experiment !!! _______________________________________________________________________________________________ My understanding is that it is P1 material. In that case every pass normalizes the immediate bottom pass. Hence code requirement for P1 FOR MANDATORY SR is 32 mm & above thickness. SOLUTION:  In any case 0. After SR=PWHT no PTC testing is required as per code--Unless for low temp. vessels. That means code ...