Skip to main content

[MW:947] RE: 865] PED Harmonised Standard for Design

EN13445 at a glance, interesting presentation

-----Original Message-----
From: materials-welding@googlegroups.com
[mailto:materials-welding@googlegroups.com] On Behalf Of Bathula
Raghuram (Mumbai - PIPING)
Sent: Saturday, June 14, 2008 10:22 PM
To: PED2000@googlegroups.com; materials-welding@googlegroups.com
Subject: [MW:865] PED Harmonised Standard for Design

Just the below link for more information, interesting one
http://www.unm.fr/en/general/en13445/

published hormonised stanadrds for Directive 97/23/EEC can be seen at
http://ec.europa.eu/enterprise/newapproach/standardization/harmstds/refl
ist/equippre.html

and
http://www.newapproach.org/Directives/ProductFamilies.asp?97/23/EC

The attached list contains references to harmonised standards for
pressure equipment and harmonised supporting standards for materials
used in manufacturing pressure equipment.

The follwoing pretext taken from a CEN link may be helpful
A harmonised standards is a standard considered by the European
Commission as satisfying some of the directives essential safety
requirements.

Harmonised standards are covered by three types of European Standard:-

* Harmonised Product Standards
These are application codes that cover the design and manufacture
of Pressure Vessels, Boilers and Pipework

* Harmonised Support Standards
Welding, NDT and other standards that supplement the application
codes.

* Harmonised Material Standards
A material specified in a harmonised standard will satisfy the
requirements of the directive in terms of ductility, toughness and
strength but does not guarantee that the material will be suitable for
a specific application.


Each harmonised standard will contain an annex stating which essential
safety requirements it satisfies. The advantage of using these
standards is that no additional justification is required that essential
safety requirements have been met and providing the standards have been
correctly applied the design of the equipment can not be challenged.

Another advantage of using Harmonised Standards is that they provide an
interpretation of the directive. For example if a pressure vessel is
to operate below zero the impact tests on the material and welding
procedures have to be carried out the lowest operating temperature the
vessel will experience according to ESR 7.5. This is not current
practice as far as either PD5500 or ASME VIII is concerned as both
these standards permit, under certain circumstances, warmer impact test
temperatures.

Harmonised Standards are not essential, any appropriate standard can
used but the satisfaction of essential safety requirements must proved.
Both PD5500 and ASME VIII have produced annexes stating how and which
essential safety requirements they claim to satisfy, these annexes have
not been approved by the European commission and therefore neither
standard can claim to be harmonised.

Note PD5500 has nothing to do with the PED, it is simply the latest
revision of BS5500, it no longer has the status of a British Standard
because it will conflict with BSEN13445. It is now a Published
Document rather than a standard, This will make no difference to it as
it will continue to be supported as long as its popularity remains

The harmonised standard for the qualification of welding personnel is EN
ISO 9606, for operating procedures it is EN ISO 15614. (Note EN ISO
15614 only satisfies the requirements of E.S.R 3.1.2 it does not
satisfy the requirements for welding consumables stated in E.S.R 4)


-----Original Message-----
From: PED2000@googlegroups.com on behalf of Rajesh
Sent: Sat 14/06/2008 17:37
To: Process Equipment Design
Cc: estamd@graphiteindia.com
Subject: [PED:93] PED Harmonised Standard for Design

Dear All,

I undrstand that Harmonised Standard For pressure vessel design for
PED is being published. BSEN13445. I have some querries.

- If this help us in selection of material.
- When this standard is likely to be published.

Regrads

Rajesh

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Re: [MW:14950] RE: 14919] Stress relieving Rejected for 5 min less soaking time.

Dear All, I have been a CONSULTANT FOR such problem & my personal opinion is expressed as follow. I fully agree with views expressed so far. But bag to differ that " Code is a law, with engineering judgments. Hence the inspector has the rights to declare that the original HT was inadequate." Inspectors & total industry must resist the "REJECTION" . We as intellectual & having seniority must become practical. How the code will revise???. ANS.: One is experiments (Pure research) & second is such chances that gives opportunity to experiment !!! _______________________________________________________________________________________________ My understanding is that it is P1 material. In that case every pass normalizes the immediate bottom pass. Hence code requirement for P1 FOR MANDATORY SR is 32 mm & above thickness. SOLUTION:  In any case 0. After SR=PWHT no PTC testing is required as per code--Unless for low temp. vessels. That means code ...