Skip to main content

Re: [MW:14609] RE: 3.2 certification


Hi,
 
Hope the attachment helps U.......
 
Cheers,
Sarav,
Korea
On Wed, Jun 20, 2012 at 2:14 PM, U WYNN-NAING <u.wynn-naing@total.com> wrote:

Dear Sir,

 

Here below is Type of Common Material Certificate Based on BS EN 10204

 

Type 2.1: Certificate of Compliance

A document issued by the manufacturer stated that the products are in compliance with the order, without any test result shown.

Type 2.2 Test Report

A document issued by the manufacturer stated that the products are in compliance with the order with test report or test result shown.

Type 3.1 Inspection Certificate

A document issued by the vendor inspection division that independent of the manufacturing department and validated by an authorized inspection representative independent of the manufacturing department.

Type 3.2 Inspection Certificate

A document issued and validated by the manufacturer's independent and authorized inspection representative with an independent authorized representative of the purchaser and or third party inspector agency validation in accordance with the Specifications of the order.

 

 

The main requirement of 3.2 certificate is all tests to be witnessed and endorsed by third party certifying agency such as BV,GL, LR, DNV, ABI etc.

Type 3.2 certificates shall state:

Name of independent inspection agency

Name of independent inspector who has witnessed the tests

The independent inspector's identification symbol and signature.

 

Rgds,

 

WN

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Bhavesh.Hansora@dnv.com
Sent: Wednesday, June 20, 2012 10:53 AM
To: materials-welding@googlegroups.com
Subject: [MW:14604] 3.2 certification

 

Dear One,

 

Can I know what is the requirement for 3.2 certification ??

 

Which are the tests to be witness by inspector ?

 

 

Bhavesh Hansora

-----------------------------------

 


************************************************************************************** The contents of this e-mail message and any attachments are confidential and are intended solely for the addressee. If you have received this transmission in error, please immediately notify the sender by return e-mail and delete this message and its attachments. Any unauthorized use, copying or dissemination of this transmission is prohibited. Neither the confidentiality nor the integrity of this message can be vouched for following transmission on the Internet. **************************************************************************************

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...