[MW:14723] Re: User acceptance of 45° Elbows

Where are you carrying out the inspection -- is it at the supplier's shop?
 
They would normally have two plates joined at right angles and machined accurate for angle and flatness.
 
The elbow with one of its ends is placed on the horizontal plate and the other end is made to meet the vertical plate's inner face.
 
Now you can actually measure or use sizewise pre-marked lines (on both the faces) to see the centre to end distance, i.e. like a gauge. This also makes it possible to check the squareness of the end.
 
However, it has its own limitations of weight, mobility, size range, wear & tear, corrosion and such other things.
 
If anybody knows any other method, pl. do share.
 
Regards
BM
 
On Friday, June 29, 2012 10:05:19 AM UTC+5:30, M. Ali Halai wrote:
Dear Experts,
 
We are usually engaged in carrying out the user acceptance inspection of various piping and fittings. Out of those, butt weld end elbows are inspected as per ASME B 16.9.
 
Now particularly the 45° Elbows are very hard to inspect due to the fact that the center to end distance given in the code cannot be easily measured as the elbow cannot stay flat on the ground and rotates according to its center of mass.
 
One way we discovered was to join two elbows end to end and measuring the face to face and comparing it to the dimensions of 90° Elbow, but still chances of error remain.
 
Any comments / suggestions are much appreciated.
 
 
Regards,
 
Muhammad Ali

On Friday, June 29, 2012 10:05:19 AM UTC+5:30, M. Ali Halai wrote:
Dear Experts,
 
We are usually engaged in carrying out the user acceptance inspection of various piping and fittings. Out of those, butt weld end elbows are inspected as per ASME B 16.9.
 
Now particularly the 45° Elbows are very hard to inspect due to the fact that the center to end distance given in the code cannot be easily measured as the elbow cannot stay flat on the ground and rotates according to its center of mass.
 
One way we discovered was to join two elbows end to end and measuring the face to face and comparing it to the dimensions of 90° Elbow, but still chances of error remain.
 
Any comments / suggestions are much appreciated.
 
 
Regards,
 
Muhammad Ali

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...