[MW:14697] Welder & process qualification ASME-IX

Dear Experts
We have client whos is welding a box structure , with one single v joint. Include angle 60 degree , root face 1.5 mm , root run Mig welding. fillup run SAW. 
Please let me know the samples required for welder qualification and process qualification and what should be the non- essential variables and non-essential variables. 
With Regards
Arijoy Roy 


From: Lakine <lakine85@gmail.com>
To: materials-welding@googlegroups.com
Sent: Monday, 25 June 2012 8:13 PM
Subject: [MW:14687] Re: Welder qualification ASME-IX

Raj,
Can we do a test coupon of 1G position and if Rt and other nde passes can he weld 6G position again or he must do a 6G test coupon to renew a 6G Welder qualification.
 of course, for renewal welder in ASME IX, they only care welding process. If they use that welding process with his range (process, thickness, diameter), position is not mention here.So, you can renewal it
On Saturday, June 16, 2012 3:21:53 PM UTC+7, raj susi wrote:

Dear experts
Good day.in Asme sec IX for welder qualification-
in my previous company I have seen that they use production weld followed by Rt to qualify a welder, but now in my new company sometimes they are using production weld and sometimes by a welder qualification coupon.
So please tell me whether we can do either way or which is best way or in which condition we should follow any of the 2 ways.
And secondly for renewal of welder qual for 6G position.
Can we do a test coupon of 1G position and if Rt and other nde passes can he weld 6G position again or he must do a 6G test coupon to renew a 6G Welder qualification.
Thanks and regards.
Raj
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...