Hi Ravi;
It is recommended to use E2553-16 or ER2553 filler metals to weld this base metal.
Regards.
K. Badri
De : Ravi Shankar <cgrtejs@gmail.com>
À : materials-welding@googlegroups.com
Envoyé le : Mercredi 2 Novembre 2011 6h10
Objet : [MW:12815] Welding Electrode
À : materials-welding@googlegroups.com
Envoyé le : Mercredi 2 Novembre 2011 6h10
Objet : [MW:12815] Welding Electrode
Dear Experts,
Please suggest me consumables for welding of Super Duplex Stainless Steel material UNS 32760.
Regards,
C G Ravi Shankar
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Please suggest me consumables for welding of Super Duplex Stainless Steel material UNS 32760.
Regards,
C G Ravi Shankar
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
No comments:
Post a Comment