Dear Patel,
Please visit www.ndt-ed.org
Best regards,
Nandesh Kumar A
From: Harry Patel <harryeng.09@gmail.com>
To: materials-welding@googlegroups.com
Sent: Wednesday, 2 November 2011 3:39 PM
Subject: [MW:12817] Welding Defect Photo
Dear Sirs,
Anybody have welding defect photo like incomplet fusion,incomplete penetration, root concavity in pipe.
I hope for your reply.