Dear Ravi Shankar
You can try with Bohler Fox CN 25 09 CuT ( SMAW) or Bohler CN 25 09 CuT-IG ( GTAW) consumables.
Data sheets attached for your reference.
Regards
Fredric Prabu
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Ravi Shankar
Sent: Wednesday, November 02, 2011 3:40 PM
To: materials-welding@googlegroups.com
Subject: [MW:12815] Welding Electrode
Dear Experts,
Please suggest me consumables for welding of Super Duplex Stainless Steel material UNS 32760.
Regards,
C G Ravi Shankar
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.