Re: [MW:33304] Pickling and passivation need before painting SS surfaces

Pickling and passivation is to remove stains and rust.

On Tue, Jul 26, 2022 at 1:14 PM srinivas rao <engr.srini@gmail.com> wrote:
when no welding or other heat applications on base metals  , no need to perfrom pickling and passivation 
regards,
srinivas Rao

On Tuesday, July 26, 2022 at 1:06:02 PM UTC+4 Abdul Qualique wrote:
Hi , 

If there is no welding done on valves then I don't find any reason for the base material to undergo Pickling & passivation. Could you please confirm if your valve is made of SA 351 CF8M.

With Best Regards,
M.A.QUALIQUE



On Tue, 26 Jul 2022 at 11:19, Anilkumar G <akg....@gmail.com> wrote:
Dear Experts

Do we need pickling and passivation of SS surfaces before painting them? Could you please suggest any specification relevant this requirement?
The parts are SS cast valves requiring painting.

Regards
Anilkumar

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/754e0d61-54e1-420e-ae4b-f92593266f5en%40googlegroups.com.

The information in this email and any associated files is confidential to Veolia Water Technologies (SASU) and/or any affiliate thereof and may be legally privileged. For the herein purposes, "affiliate" means any legal entity, partnership, joint venture, equity, company, including in particular any and all subsidiary which, directly or indirectly, controls Veolia Water Technologies (SASU) and/or is under the control thereof and/or is under the control of the ultimate parent company thereof, and "control" means the ability to directly or indirectly, direct the affairs of a third party by means of ownership, contract or otherwise. It may also contain information that is subject to copyright or constitutes a trade secret. It is intended solely for the named recipient. Access to this email by anyone else is unauthorized.

If you are not the intended recipient, please note that any use, disclosure, copying, distribution of this email or any action taken or omitted to be taken in reliance on its prohibited.

Warning: Although this email and any attachment thereto are believed to be free from viruses, it is the responsibility of the recipient to ensure that they are virus free. No responsibility whatsoever is accepted by Veolia for any loss or damage arising from their receipt or opening.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/a839820e-b07d-4953-abb8-8bd0de9b322cn%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAFycdMw1w5yye0aD1MCfB3oz2j7w6A4p_ZgLsoBYCKtBKeV%3Dow%40mail.gmail.com.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...