Re: [MW:33211] Toque Range Chart - Stud & Nuts

Dear Sir,

Consider my reply marked in blue

Williams,
What is it that you are bolting? - Flange End Pipe Spools (Photo attached below)
Flange Type - WNRF & RTJ 
Plated or unplated?  - Unplated 
Lubricated? Type? K factor? - Stud & Nut - Mill Test certificate is attached below FYR
Gasket type? - SPW & Rig Gasket
Are you trying to achieve maximum amount of tightness shy of reaching the yield of bolting material? Or sufficient amount of compression/clamping on a specific type of gasket material? 

Thanks,

Chip Frizzell 

Quality Manager 

CWI / ASNT NDT LVL III / CRI / NACE CIP LVL 2-Certified

CELL: 520-510-8093

Price is what you pay-value is what you get. 
Seldom does the lowest price result in the best value!

Sent from my iPhone

On Jul 6, 2022, at 1:56 AM, williams p wilson <williamswilsonp@gmail.com> wrote:


Dear Experts,

If anybody has the Torque range chart for Stud & Nuts - Please share.
Material - ASTM A 193 B7  & ASTM A 194 Gr.2H

Thank You & Regards
Williams P Wilson
QA/QC Engineer
Welding Inspector (CSWIP 3.1)
Cell: (+968) 94600828
P Please consider the environment before printing this message

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHBxnQ4pbFpz%3D3E9oM-Hp%2B4%3DzVrTBrWPjFC4NxSds1fp%2BJTt2Q%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/8D41DED6-1F78-4FCC-98C9-E11559BCA2C4%40gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHBxnQ7bQex33YOhheV2kOvGcS1QS%2BV--NKNyGxWSXLe9O7xqg%40mail.gmail.com.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...