Dear All, I have one doubt, 

in wps there is a line Pulsing current --------in the format. If i prepare new wps , what to write there -- if I process SMAW? IF process GTAW, IF process SAW, IF process GMAW? can i one tell for each process.

On Fri, 15 Jul 2022 at 11:43, Vishwas Keskar <vvkeskar123@gmail.com> wrote:
 Hope this is Carbon steel dished end.
First discuss with Design Engineering about this  chordal joint in dished end.
Then locate the joint based on plate width.
Get the drawing.
Check with Dished end forming expert , Is this dished end is  cold forming or hot forming. 
Based on forming Method,  select WPS.
Finalise proposal in consultation with 
Methods Engineering, Design Engineering,  QA and Manufacturing. 
Accor. prepare QAP  Method statement  and circulate to Mfg as per ISO issue document 

Vishwas 
IWE -
International Welding Engineer



On Fri, 15 Jul 2022, 11:29 CKML, <chaitanyakamal@gmail.com> wrote:
Dear Experts 

 Can i proceed forming of 30 mm thk Plate by joining of 2 Plates for  Lower shell dish end.

If cant what would be the acceptable of joining length of plates.
If yes what precaution to be take care.

Any reviews 

can any one help me 

Regards
chaitanya kamal 
ph-8226081506  



--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/57bd9e9a-da16-4e1c-ba2b-dc806d01205bn%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADder3ODHZpqRtJfyJiYERMRfAefyAOE_-U%3DF2VXZDxvwE5-5A%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALUa47huqUY8ih7DRehEEri4797kZ1EiCRg%2Bt5FWZ0ZtPhe5ZA%40mail.gmail.com.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...