Skip to main content

Re: [MW:33244] WELDER QUALIFICATION REQUIERMENT

Choose a higher thickness pipe say 20mm wherein you can weld GTAW 5mm (2t) and SMAW 15mm with minimum 3 layers so for SMAW he will be qualified for unlimited thickness and say GTAW 10mm/

Thanks & Regards

J.Gerald Jayakumar



On Thursday, 14 July, 2022 at 05:09:42 pm IST, Adnan Ziad <adnanziad49@gmail.com> wrote:


In our case he weld 5 mm gtaw + 9.27 mm smaw 

Can i qualify him directly on the two wps 

On Thu, Jul 14, 2022, 12:09 'james gerald' via Materials & Welding <materials-welding@googlegroups.com> wrote:
What you have mentioned is Basemetal thickness but in Welder qualification only weld metal thickness is an essential variable qualified from 0 to applicable weld metal thickness for each process, BM thickness is unlimited

Thanks & Regards

J.Gerald Jayakumar




On Thursday, 14 July, 2022 at 01:18:52 pm IST, QA/QC <adnanziad49@gmail.com> wrote:


Dear Experts

i have two wps's for piping cs/ltsc welding with the asme b31.3 ans sec 9  one thickness range is 3 to 20 mm and the second is 20.01to 31.22  pwht requiered .the two is GTAW+SMAW

i have a welder qualify in test coupon 6'' 14.27 mm 

my question is this welder will qualify to weld in the two wps or we should make another qualification for him seperately 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/083762d2-dd64-482a-85e9-0e4f7aa4e14bn%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1357071013.761925.1657796938751%40mail.yahoo.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CACbfGKfUAWSWQBvotP2q78PrFFKk5eqBCem3vh-a2pvEbvbAqQ%40mail.gmail.com.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...