Share details of drawing requirement & application to have clarity on electrode selection
On Wed, Mar 20, 2019, 3:23 PM Bien ND <bck055@gmail.com> wrote:
Did you run a test coupon?--How is the test result, chemical and mechanical test?
Vào 13:33:36 UTC+7 Thứ Ba, ngày 19 tháng 3 năm 2019, Chintan đã viết:Use ER 316 or ER 2594 for builtup / buffer layer
Max interpass temp 150 deg cel
Use durmat NiFD wire for tugsten carbide hardfacing over p550 ( use er316 as buffer layer)
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to a topic in the Google Groups "Materials & Welding" group.
To unsubscribe from this topic, visit https://groups.google.com/d/topic/materials-welding/EkeUuiTQaTA/unsubscribe.
To unsubscribe from this group and all its topics, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.
Comments