Re: [MW:29392] Qualification of 2 welders in one Test Piece (Pipe 12" inch)

Sir,

As per the code is YES. 

But as per the ASME IX  interpretation, the welder should complete one full circumference weld. 

I remember when we doing the qualification, our client insist to do full circumference weld w.r.t to this class.

I am searching for the interpretation No and clause. I will send to you.

Regards

Pramodh M.R
Sr. Inspector (welding/coating)

If We Work With Determination And Perfection, Success Will Follow



On Tuesday, March 26, 2019, 1:39:26 PM GMT+3, 'Ibrahim Ramadan Hassan' via Materials & Welding <materials-welding@googlegroups.com> wrote:


If the Position of the WQT is 6 G , that one Test coupon (12 " inch ) - Can qualify Two welders or Not ? hence the total length welded by the two welders in parallel
 will be radio graphed.

Best Regards
Eng. / Ibrahim Ramadan Hassan
Section Head Mechanical QA/QC
PETROJET - Jordan Branch
Egypt Mob. : 00201000948366
Jordan Mob. : 00962791023621






On Tuesday, March 26, 2019, 9:37:50 AM GMT+2, chandraknat vaidya <vaidyac10@gmail.com> wrote:


Yes. Provided All other essential variables should same.
CLV

On Tue, Mar 26, 2019 at 7:59 AM George Dilintas <dilintas@gmail.com> wrote:
It depends also on the positions you want to qualify. Pls read the Code carefully, to check if they have to weld an entire circumference

Στις Σάβ, 23 Μαρ 2019 στις 2:07 μ.μ., ο/η 'Ibrahim Ramadan Hassan' via Materials & Welding <materials-welding@googlegroups.com> έγραψε:
Dear Sir
I am inquire about the Welders qualification test as Per ASME IX - QW-302 & QW-304
If I make WQT for qualification of (2) welders welding together in one test Pipe 12 " inch
hence the total circumference of Pipe 12 " inch = 957 mm so, Each welder will weld more than 150 mm as required by ASME IX And all the Pipe Circumference welded by each welder will be radio graphed.
Is that Acceptable is or not to qualify 2 welders in one test piece (Pipe 12" inch)?

Kindly reply on my inquiry.

Best Regards
Eng. / Ibrahim Ramadan Hassan
Section Head Mechanical QA/QC
PETROJET - Jordan Branch
Egypt Mob. : 00201000948366
Jordan Mob. : 00962791023621




--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.



--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...