Skip to main content

Re: [MW:23280] Multiple WPS from single PQR

Many advantages like:
1. Partial penetration welds
2. Combination with other processes 
3. Welding of small bore piping with GTAW


Sent from my BlackBerry 10 smartphone.
From: Ri@z
Sent: Πέμπτη, 6 Αυγούστου 2015 - 13:24
To: Materials & Welding
Reply To: materials-welding@googlegroups.com
Subject: Re: [MW:23276] Multiple WPS from single PQR


Thank You For reply


My humble doubt is, 1 ) weld metal deposition is restricted to be max 6 mm for gtaw, and 13 mm for SMAW, what is the advantage of having 19 mm as  Qualified base metal thickness. For separate process there is no advantage of Base metal Qualified as per QW-451 ie 1.5 to 2T

AM I RIGHT ???


On Thursday, 6 August 2015 14:02:14 UTC+5:30, George Dilintas wrote:
Backing is a welders qualification essential variable. For PQR it is a nonessential one.
The Base metal qualification range is the same for the 3 cases

Sent from my BlackBerry 10 smartphone.
From: 'Bijay' via Materials & Welding
Sent: Πέμπτη, 6 Αυγούστου 2015 - 09:55
To: materials-welding@googlegroups com
Subject: Re: [MW:23273] Multiple WPS from single PQR

But for SMAW single process you have to give Metal baking as the GTAW weld Metal act as metal baking.

Sent from Yahoo Mail on Android


From:"Ri@z" <riaz.r...@gmail.com>
Date:Thu, 6 Aug, 2015 at 11:58 am
Subject:[MW:23271] Multiple WPS from single PQR



Dear Sir,,


I have one PQR with 3 mm GTAW weld deposit and 6.5 mm SMAW deposit. Base metal thickness is 9.5 mm and impact is not required.

Please correct me if any of the following is NOT correct as per Sec IX

1) Combined Process (GTAW + SMAW) up to a thickness of 1.5 to 19 MM (2T)

2( Single process wps of SMAW with weld metal thicjness 13 MM and qualified base metal thickness is 1.5 mm to 13 mm

3)  Single process WPS of GTAW  with weld metal thickness of 6 MM and Qualified base metal thickness is 1.5 to  6 mm




Please help!!

Riaz 

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/b3a24345-befb-4d5c-b65a-9cfc47a53889%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1438843327.97025.YahooMailAndroidMobile%40web181301.mail.ne1.yahoo.com.
For more options, visit https://groups.google.com/d/optout.

This message contains confidential information. To know more, please click on the following link: http://disclaimer.bureauveritas.com

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/cba069da-c9e1-4902-9e1d-bbefd56859c0%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.


This message contains confidential information. To know more, please click on the following link: http://disclaimer.bureauveritas.com

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...