Skip to main content

[MW:23269] Re: Economizer tube crack

jian xu, thanks for your valuable response,

 

        We have a 6 boiler, same economizer inlet header tube leak at tube to header joint leak,

The header thickness is 18mm and tube is stub in 7mm in header,

I attached a one report which is generated early,

Can you give your valuable suggestion of this failure?



On Friday, July 17, 2015 at 1:37:38 PM UTC+3, Jian Xu wrote:


在 2015年7月16日星期四 UTC+8下午2:28:52,Mian gee写道:
Dear All, please support to investigate the crack of ecanomozer tube.as
attached picture

    Type of tube- spirlly finned tube
     spiral material-sa-178a
     tube dia meter-219.1mm
      tube material-106b
       Maximum design pressure-5800kpa
     

Hi,

This photo don't provide enough information, first, confirm with some details.
1.you sure the leak point is cracking? or just like localized loss of thickness?
2 if localized loss of thickness, if other area have the same issue, or loss of thickness phenomena. if so, you should take care the corrosion issue, review the composition of the medium.
3.if leakage is due to crack, then you should distinguish crack the position where on the weld or along the HAZ, welding quality should be paid more attention. Also, excessive temperature in localized area is another potential reason.
In the end, I suggest more detailed investigation on other similary area is necessary action.
Thank you! 

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/337f9cf1-ffd3-4a51-84a9-25ce1414d55a%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...