[MW:20405] ASME Sect IX-QW-405-Position Qualification Ranges

Dear Experts

Position only a Supplementary essential variable (ie when CVN-Impact test required).

QW-405.2 A change from any position to the vertical position uphill progression. Vertical‐uphill progression
(e.g., 3G, 5G, or 6G position) qualifies for all positions. In uphill progression, a change from stringer bead to weave
bead. This variable does not apply when aWPS is qualified with a PWHT above the upper transformation temperature
or when an austenitic material is solution annealed after welding.

QW-405.4 (a) Qualification in the horizontal, vertical, or overhead position shall also qualify for the flat position. Qualification
in the horizontal fixed position, 5G, shall qualify for the flat, vertical, and overhead positions. Qualification in
the horizontal, vertical, and overhead positions shall qualify for all positions. Qualification in the inclined fixed position,
6G, shall qualify for all positions.

I'm looking at some of the WPS/PQRs received from Vendor. 
PQR state that Position Tested/Qualified- 1G
WPS state qualified for all groove and fillet positions?
CVN Tested at -30 deg C.

Based on QW-405.2 & QW-405.4- 1G does not qualify all positions.Only qualified for 1G & 1F.

Plls explain how "This variable does not apply when aWPS is qualified with a PWHT above the upper transformation temperature
or when an austenitic material is solution annealed after welding." relevant to Positions.


Pls shine some light on this. Thank You.



















































--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:30043] Weep hole

If weep hole is not provided in dummy pipe before welding What will happen??? -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/da251ee6-fa7f-4851-b876-cdb3834ae341%40googlegroups.com .

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .