Skip to main content

Re: [MW:19419] special UT procedure inspection for small pipe diameter and high thickness

dear all
this second mail for you please answer me i want to guide.
please i want to how do  special UT procedure inspection for small pipe diameter and high thickness and if you have procedure copy to guide me.
the requirement of Client / Specification depend on ASME code because all piping work is high gas small bore up to  6" and thickness up to 11.3mm carbon steel and alloy steel P91 and P11. 
regrades.


On Mon, Nov 25, 2013 at 8:58 AM, Shipo shipo <shipo.ptj@gmail.com> wrote:
dear P Govindan
 
thank you for answer and the requirement of Client / Specification depend on ASME code because all piping work is high gas small bore up to  6" and thickness up to 11.3mm carbon steel and alloy steel P91 and P11. 


On Sun, Nov 24, 2013 at 5:03 PM, Perumal Govindan <perumalgovindan@gmail.com> wrote:
Mr. Shipo,

Find out the requirement of Client / Specification. Once known the Client requirement we may write a special UT procedure, after referring Codes and Standards.

P Govindan


On Sun, Nov 24, 2013 at 12:31 PM, Shipo shipo <shipo.ptj@gmail.com> wrote:
dear all
please i want to how do  special UT procedure inspection for small pipe diameter and high thickness and if you have procedure copy to guide me.
--
     
     BEST REGARDS

    SHAABAN MOHAMED ALI SOLIMAN
      QA/QC DEPARTMENT
     PETROJET MARINE DEPARTMENT
     Mobile: +2 012 27 02 44 53

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.



--
     
     BEST REGARDS

    SHAABAN MOHAMED ALI SOLIMAN
      QA/QC DEPARTMENT
     PETROJET MARINE DEPARTMENT
     Mobile: +2 012 27 02 44 53



--
     
     BEST REGARDS

    SHAABAN MOHAMED ALI SOLIMAN
      QA/QC DEPARTMENT
     PETROJET MARINE DEPARTMENT
     Mobile: +2 012 27 02 44 53

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

Comments

Popular posts from this blog

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...

[MW:5202] RE: 5200] NDT after PWHT

------------------------------------- Interpretation:  I‑89‑14 Subject:         Section I (1986 Edition, 1987 Addenda), PW‑11,                  NDE Prior to PWHT Date Issued:     December 15, 1988 File:            BC88‑393   Question: Does PW‑11 require that NDE be performed on welds after they have been subjected to the postweld heat treatment required by PW‑39?   Reply: No, unless the conditions described in PW‑11.2.2 exist. ---------------------------------------------- Interpretation:  VIII-1-98-09 Subject:         Section VIII, Division 1 (1995 Edition, 1996 Addenda); NDE                 ...

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...