[MW:19405] RE: 19400] Duplex Stainless Steel: Metallurgy, engineering codes & welding practices

The correction to these mistakes will appear as "errata" in the 2nd part of this article.
 
Thanks
 
Pradip Goswami, P.Eng,IWE
Welding & Metallurgical Specialist
Ontario, Canada
 
 


From: pgoswami [mailto:pgoswami@quickclic.net]
Sent: Friday, November 29, 2013 7:34 AM
To: 'Raghuram Bathula'; 'Raghuram Bathula'
Cc: 'materials-welding@googlegroups.com'
Subject: FW: 19400] Duplex Stainless Steel: Metallurgy, engineering codes & welding practices

Mr... Bathula,
 
Thanks for your appreciation.Although we took enough care to write a good article, some editorial mistakes in the paper did occur. Other than those this paper (a review article) should be worth reading and enjoying.
 
Regards.
 
Pradip Goswami, P.Eng,IWE
Welding & Metallurgical Specialist
Ontario, Canada
 
 


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Raghuram Bathula
Sent: Friday, November 29, 2013 3:52 AM
To: Materials-Welding
Subject: [MW:19400] Duplex Stainless Steel: Metallurgy, engineering codes & welding practices

Congratulations Mr Pradip Goswami for the article in current issue of SSW

Duplex Stainless Steels (DSS) are extremely high grade engineering alloys combining good corrosion resistance with high strength and ease of fabrication. These steels are frequently used in the oil and gas industries both in upstream and downstream applications for assemblies such as pipe work systems, manifolds and risers. Furthermore, these are used in the petrochemical industry in the form of pipelines and pressure vessels. These steels are designed to provide better corrosion resistance, particularly chloride stress corrosion and chloride pitting corrosion, in addition to having a higher strength than standard austenitic stainless steels such as Type 304 or 316, enabling thinner sections to be used and providing significant cost benefits.

By Ramesh Bapat, Senior Principal Engineer, Foster Wheeler Upstream & Pradip Goswami, P. Eng., IWE, Welding and Metallurgical Specialist - Ontario, Canada

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

Comments

Popular posts from this blog

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...

[MW:5202] RE: 5200] NDT after PWHT

------------------------------------- Interpretation:  I‑89‑14 Subject:         Section I (1986 Edition, 1987 Addenda), PW‑11,                  NDE Prior to PWHT Date Issued:     December 15, 1988 File:            BC88‑393   Question: Does PW‑11 require that NDE be performed on welds after they have been subjected to the postweld heat treatment required by PW‑39?   Reply: No, unless the conditions described in PW‑11.2.2 exist. ---------------------------------------------- Interpretation:  VIII-1-98-09 Subject:         Section VIII, Division 1 (1995 Edition, 1996 Addenda); NDE                 ...

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...