The purposes of preheat are to avoid crack due to sudden heating and for wide heat affected zone,so in my openion preheating is required for both cutting and welding.
 
Regards,
 
Sandeep.M.V
 


 
On Tue, Jan 17, 2012 at 10:31 AM, Lakshman Kumar.B <lakshmankumar4@gmail.com> wrote:

Dear All,

 Beyond all the technical aspects, small logic for this situation….

This is only my view…

 

After cutting the edges are again welding to some part / connection(say pipe, fitting, flange, etc or leaving like that) in all the cases if welding is going to do it will be again preheat and PWHT after welding so any thermal shocks will be relived during PH, PWHT,

 

So I think no need of pre heating.

 

Thanks and Regards................?

 

Lakshman Kumar.B|Manager |Lanco Infratech Limited

Plot No 1255 | Sanjeevani chowk | Mahanadi vihar | Cuttack 753004

Phone : + 91 671 2445033 | Mobile : +91 9937286851 |www.lancogroup.com

Go Green|The future will thank you

 

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of jesti fer
Sent: Monday, January 16, 2012 3:22 PM


To: materials-welding@googlegroups.com
Subject: [MW:13484] Pre-heating for cutting

 

Dear Experts,

 

I need your help for this subject, We are fabricating some piping as per B31.3, the material ASTM A106 Gr.B, 8"Sch-XXS and 160 and we are doing preheat and PWHT for welding, but my enquiry pre heat is required for cutting also? It is mentioned in any code or any other were? Please help me

 

Jesti

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

[MW:30043] Weep hole

If weep hole is not provided in dummy pipe before welding What will happen??? -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/da251ee6-fa7f-4851-b876-cdb3834ae341%40googlegroups.com .