Skip to main content

[MW:13569] Re: need your help please : Can I take CSWIP 3.2 without hold CSWIP 3.1 ?

Mohammed Maher,

You can do CSWIP 3.2 with out attending CSWIP 3.1

But You have to attend CSWIP 3.1 exam then immediately the day after
you can sit CSWIP 3.2

Once if you passed CSWIP 3.1 then only TWI allows you to attend CSWIP
3.2

I am Navaneetha from England,

My suggestion is CSWIP 3.1 is not at related to expeience. Even 15
years experience holder in Welding usually fails in CSWIP 3.1

The Unique of CSWIP 3.1 is Measuring & Recording the Weld defects, Its
like a Police Training.

How much knowledge you have to cathch the weld defects.

So bettet attend CSWIP 3.1 & wait for one year.Then attend CSWIP 3.2

In CSWIP 3.2 you have good & deep knowledge in Heat Treatment, RTFI
otherwise CSWIP 3.2 is Big bang for you

Best of Luck

Regards
NAV

On Jan 22, 12:08 pm, mohamed maher <mohamed.ahmed.ma...@gmail.com>
wrote:
> dear, all
> I need to take CSWIP 3.2 but I am not certified CSWIP 3.1 and
> according to Requirements for the Certification of Visual Welding
> Inspectors, Welding Inspectors and Senior Welding Inspectors (fusion
> welding) - (Document No CSWIP-WI-6-92 11th Edition September 2011).
> Implementation Date September 2011 ,
>  I can take CSWIP 3.2 directly with no need to be certified with CSWIP
> 3.1 if i have 5 years experince .
>
>   My question now , I  want to take the exam of CSWIP 3.2 and I am
> not certify with CSWIP 3.1 and I have more than 6 years experince .
>
>  Thank you for your time and consideration ,Looking forward to hear
> from you.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...