BS 7570 is no longer valid but replaced by EN 50504.
Met vriendelijke groeten / Best Regards
Herman Pieper
Pieper Quality Support & Inspection
Phone: +31 (0)521 380083
Fax: +31 (0)84 7539225
Cell: +31 (0)6 51691215
www.pieper-qsi.nl
Van: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] Namens Madhusudan Rout
Verzonden: dinsdag 1 november 2011 15:23
Aan: materials-welding@googlegroups.com
Onderwerp: Re: [MW:12811] Welding Machines Calibration
Follow the BS-7570 standard for callibration.
if you need the standard , i can sent you.
On Mon, Oct 31, 2011 at 4:52 PM, Tarek Yehia <t.yehia2009@gmail.com> wrote:
Dear Experts,
can any body tell me what is the recommended procedure for a/m subject and provide me with some written procedure or work instruction but should be based on applicable standard or suitable reference.
--
Best regards,
Tarek Yehia
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
No comments:
Post a Comment