Skip to main content

Re: [MW:7291] Can we do painting prior to hydrotest?

Dear Mr.Satish
 
You may give a go ahead by considerably increasing the holding time, could be double the time specified by the spec while you also consider other factors of safety and design.
 
Regards
 
J.N.Murthy
Engg.QA/QC.

On Thu, Sep 30, 2010 at 2:47 PM, Satish Hingalkar <shingalkar@gmail.com> wrote:
Hi,
 
Thanks a lot, i search in ASME B31.3 below bold sentence,but i couldn't find,can u please help me for this.,where it is exactly so that i can decline this deviation.
 
Please help me if possible uregently because my PM pressuring me to reply that will be appreciated.
 
Waiting for reply.
 
Regards,
Satish

On Thu, Sep 30, 2010 at 1:33 PM, Bathula Raghuram (Mumbai - PIPING) <R.Bathula@ticb.com> wrote:

Interesting, and you have a valid point but nothing is proven, until then just go with the flow (tried and tested methods). No Inspector would be happy but bound to accept as per code.  remember your company specification prohibits it and you are intended to accept, hence code reference is given, Masking of any discontinuity by thin layer of paint, may be yes perhaps may be not. If you refer the paragraphs of these codes which will give a cautionary statement at the end "painting/coating may mask the leak".

Normally weld joints are left open and rest of the area is painted before hydro.

In my opinion 105 bar is too high for a layer of paint to with stand, or you may allow only blasting and priming before hydro and final coating after hydro. If I remember correctly only Australian code AS1210 prohibits it.

 

From: Satish Hingalkar [mailto:shingalkar@gmail.com]
Sent: Thursday, September 30, 2010 12:49 PM
To: Bathula Raghuram (Mumbai - PIPING)
Subject: Re: [MW:7283] Can we do painting prior to hydrotest?

 

Hi,

 

Thanks for prompt reply

Piping system of having pipe rack near about 4 KM,service-Nitrogen,Code ASME B31.3

 

As u said,ASME B 31.3 allows,but my query is that whether painting will affect the joint leak detection normally found in hydrotest??

 

As per my knowledge,Painting has ability to penetrate and plug/ seal off small pin holes which are normally detected in hydro test.      After curing, paint can withstand pressure in small pin holes that can obstruct the leaks. But during operation, paint can be decomposed and start leaking,please comment.

 

Regards,

Satish

On Thu, Sep 30, 2010 at 7:27 AM, Bathula Raghuram (Mumbai - PIPING) <R.Bathula@ticb.com> wrote:

You have not specified the type of component, fluid and design code.

ASME code for both vessels and piping have this provision. Sec VIII div 1 allows except for lethal service (UG 99) and B31.3 allows except for sensitive leak testing (345.3.1)

 From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Satish Hingalkar
Sent: Wednesday, September 29, 2010 11:55 PM
To: Materials & Welding
Subject: [MW:7276] Can we do painting prior to hydrotest?

 Dear Members,

 Our contractor has raised a design change request for painting prior to hydrotest.As per COMPANY specification,painting to be carried out after successfull complection of hydrotest,but contractor wants to do painting before hydrotest,can we accept this deviation? if  we want to accept the deviation,what criteria to be follow??

 Our design conditions are 105 barg hydrotest pressure and design temp.85 deg.c,NDT is 10% MT & 10% RT.

 Waiting for reply.Pl.respond ASAP.

 

Regards,

Satish


 


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...