Hello Syed,

 

Materials for sour service should comply with the requirements of MR-0175.My understanding is that what NACE calls for that both manufacturer/supplier and the purchaser should be in compliance.

 

Purchaser or end users compliance is to specify the details as asked in Annex-E(see below).

 

Supplier/Manufacturer’s responsibility : Although there is no direct reference to supplier/fabricator responsibility in MR0175/ISO15156 the following sections imply responsibility.

  • cooperate and communicate in an exchange of information between the end users and materials suppliers/manufacturers concerning required or suitable service conditions. ( Clause 5. to 5.5-Purchasing requirements)
  •  ensure the material purchased meets the end users requirements and the requirements of the standard. (Clause 7.0  and others, especially hardness and all required manufacturing requirements)

Both API-5L and ASTM A-106 are NACE accepted materials, which means they had undergone various qualification and acceptance steps, plus the service history in similar environment to be accepted. Hence they are very known material in sour environment. So material may not be a bothersome issue.

However at the first place if your P.O and other related contract documents calls for conformance to MR-0175, then the supplier has to conform to this and specify the same in the paperwork..

As you stated below: -But still they deny to declare  the compliance with NACE MR0175/ISO 15156, they say that  ‘’ Only hardness according to NACE MR0175/ISO15156’’ will be reported on mill test certificate. This does not sound convincing, looks some wishy washy stuff???

 

MR-0175 calls for:-Materials complying with this part of NACE MR0175/ISO 15156 shall be made traceable, preferably by marking, before delivery. Suitable labeling or documentation is also acceptable.

 

May be it's good  to ask the supplier why this deviation? before accepting the material.

 

I think I've my best to clarify your doubt. Further you may use the attached guide for your future references on MR-0175.This document is an useful guidebook but  without any liability.

 

Thanks.

 

 

Pradip Goswami,P.Eng.
Welding & Metallurgical Engineer/Specialist
Email-pgoswami@sympatico.ca,
 
 

  

cid:1.1369525492@web55807.mail.re3.yahoo.com

 

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of DOKKU AJAY
Sent: Wednesday, September 29, 2010 9:44 AM
To: materials-welding@googlegroups.com
Subject: Re: [MW:7269] NACE MR0175

 

Resent, please ignore earlier e-mail as it was incomplete.

 

Hello Moin,

 

As the requirements from NACE MR 0175 specified by you had been agreed by the material manufacturer & the values will be stated in the MTC, solves your problem.

 

i.e the MTC shall state all the test results, i,e hardness, nickel content, Heat-treament condition. If all the conditions are acceptable as per Annexure-A.2, then the material can be accepted.

 

Please refer Clause 9 of Annexure -2, which states that "Suitable labelling or documentation is also acceptable". Hence MTC documenting the requirements is sufficient to accept the material.

 

I hope it was clear.


 

Dokku Ajay Kumar

 

Dokku Ajay Kumar
Mobile: +966 500071054

 

 


From: Moin - QC <Syed.Moin@gerabgroup.com>
To: materials-welding@googlegroups.com
Sent: Tue, September 28, 2010 4:30:48 PM
Subject: RE: [MW:7253] NACE MR0175

Dear Pradeep,

 

Thanks for information,

 

Material we intent to purchase is API 5L line pipes and A106 pipes for SOUR service, these  product specification are listed in NACE MR0175.

 

Manufacturer has confirmed that Value of nickel content on product analysis will be less than 1%, Sulphur will be 0.004% Maximum,  CE value will be less than 0.38 and material will be supplied in ‘’ Normalized formed’’ condition.

 

But still they deny to declare  the compliance with NACE MR0175/ISO 15156, they say that  ‘’ Only hardness according to NACE MR0175/ISO15156’’ will be reported on mill test certificate.

 

I was trying to find out the restriction NACE MR0175 set forth for API 5L and A106  material, all I could find was restriction on nickel, sulphur and delivery condition(i.e. hot forming or Normalizing etc) which have been complied with by the manufacturer, but still they deny to declare the compliance with NACE MR0175 which left me confused.

 

Could you please put some light on this issue.

 

 

REGARDS,
SYED MOIN

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of pgoswami
Sent: Monday, September 27, 2010 5:48 PM
To: materials-welding@googlegroups.com
Subject: RE: [MW:7227] NACE MR0175

 

Hello Syed,

 

If you look at the end of MR-0175,Part-2, 2003-version, the list of accepted materials for sour service are listed. There are specifications for a few seamless pipes also.

 

Coming back to your query: Material According to NACE MR0175’’—Implies that all the requirements of MR-0175 have been met by the manufacturer and the material is fit for sour service. If one goes through in details, MR-0175 provides the guidelines of what tests to be asked for sour services. See the sample below-ANNEX-E.

 

The second option specified by your manufacturer:- Hardness according NACE MR0175—does not make any real sense, this means they would conform to 22 HRC(248VHN) hardness requirements as required by the spec at the point of supply.

 

What’s the specification of Pipes to be purchased??. If it’s covered in MR-0175then the supplier has to stick a manufacturing and Q.A program meeting NACE MR-0175.If it’s newer materials, it requires qualification to MR-0175.

 

It would be good if you read the MR-0175 and specifically ask for the applicable clauses, for your application, then it will put the mills on the hook.

 

Thanks.

 

Pradip Goswami,P.Eng.

Welding & Metallurgical Engineer/Specialist

Email-pgoswami@sympatico.ca,

pgoswami@quickclic.net

 

 

5 Purchasing information

5.1 The preparation of material purchasing specifications might require co-operation and exchange of data between the equipment user, the equipment supplier and the material manufacturer to ensure that the material purchased complies with NACE MR0175/ISO 15156-1 and this part of NACE MR0175/ISO 15156.

5.2 The following information shall be provided:

·          preferred material types and/or grades (if known);

·         equipment type (if known);

·          reference to this part of NACE MR0175/ISO 15156;

·          acceptable bases for selection of materials for SSC resistance (see Clause 7);

·          requirements for HIC resistance (see Clause 8).

5.3 The equipment user and the equipment supplier/material manufacturer may agree that carbon or low alloy steels other than those described and/or listed in Annex A may be selected subject to suitable qualification testing in accordance with Annex B and NACE MR0175/ISO 15156-1. The qualification requirements may be extended to

include resistance to SOHIC and SZC.

If the purchaser intends to make use of such agreements, extensions and qualifications, the appropriate additional information shall be clearly indicated in the materials purchasing specification. This information may include

·         requirements for SSC testing (see 7.1, 7.2),

·         service conditions for specific sour service application, and

·         other special requirements.

5.4 Annex C describes how to calculate the H2S partial pressure and Annex D gives guidance on how to determine the pH-value of a fluid.

5.5 The information required for material purchasing shall be entered on suitable data sheets. Suggested formats are given in Annex E.

 

 

 

 


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Ramprasad Chari
Sent: Monday, September 27, 2010 12:00 AM
To: materials-welding@googlegroups.com
Subject: Re: [MW:7209] NACE MR0175

 

If the mill supplying a seamless pipe is pre-qualified to supply NACE pipes,you need not carry out SSC test.Mill shall indicate NACE conformance on their TC including Hardness values.Everything depends on the customer's requirements.Many a times it is seen that Gas/liquid is not 'sour' with partial pressure of H2S so low that  NACE does not apply but still customer insists for NACE conformance.As I have indicated in my previous mail,if your customer permits you,you can carry out SSC test on a pipe as per TM0177 standard and conform Nace compliance through lab test reports including hardness.You can go one step further and get micro test done as per ASTM E-45 method D and confirm absence of 'elongated MnS inclusions'.If the mill confirms NACR compliance,you do not have to carry out any other tests unless your customer has asked you additional specific tests.

Regards

Aarpee

On Sat, Sep 25, 2010 at 6:03 PM, Sivashankar Nagamanickamsundaramoorthy <poovaishankar@yahoo.com> wrote:

Hi Mr.Aarpee,

 

 Wheather SSC test is required for the Seamless pipes for the confirmation to the  NACE requirements ?.

 

 

Regards

 

Siva

 


From: Ramprasad Chari <ramprasad.chari@gmail.com>
To: materials-welding@googlegroups.com
Sent: Thu, September 23, 2010 1:48:58 PM
Subject: Re: [MW:7171] NACE MR0175

 

Conformance to NACE MR0175 certifies material to be used for 'sour' gas applications which implies that material is resistant to various cracking mechanisms assoiated with H2S presence in a wet gas/liquid.If the mill is pre-qualified carrying out tests as per TM0177 standard(for SSC) and TM0284(for HIC) then mill can certify conformance.Alternatively,if the client permits you can carry out the test per heat per size to confirm conformance to NACE MR0175.For seamless pipe HIC may not be required but for welded pipe,you may have to carry out HIC as well as SSC test.Hardness is one of the criterion of max 22HRC.If hardness is not achieved in 'as 'condition in weld and HAZ,you may have to carry out PWHT to ensure that hardness is below 22 HRC.

Regards

Aarpee

On Thu, Sep 23, 2010 at 10:53 AM, Moin - QC <Syed.Moin@gerabgroup.com> wrote:

Hi,

Can somebody please explain the difference between ‘’ Material According to NACE MR0175’’ & ‘’ Hardness according NACE MR0175’’

I am purchasing some material from mill, but they said that they can meet the hardness requirement only, but cannot write ‘’ Material accordance to NACE MR0175’’ on material test certificate.

Material is seamless and welded pipe.

Thanks & Regards
SM


______________________________________________________
CONFIDENTIALITY NOTICE: This electronic mail transmission may contain information that is confidential, privileged, proprietary, or otherwise legally exempt from disclosure and is intended only for the use of the recipient named above. We do not waive confidentiality in the event this mail was transmitted wrongly. If you have received this communication in error, and are not the intended recipient, you are hereby notified that you are prohibited from reading, printing, copying, or disseminating this message, any part of it, or any of the attachments it may carry. If you have received this message in error, please destroy all electronic and paper copies and notify the sender immediately of the inadvertent transmission. We would like to advise you that we would not waive any of our privilege for taking action against you in the event the confidentiality of this message has been compromised. Thank you for your cooperation
________________
This email has been scanned by the MessageLabs Email Security System.
For more information please visit http://www.messagelabs.com/email
______________________________________________________________________

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please visit http://www.messagelabs.com/email
______________________________________________________________________

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


______________________________________________________
CONFIDENTIALITY NOTICE: This electronic mail transmission may contain information that is confidential, privileged, proprietary, or otherwise legally exempt from disclosure and is intended only for the use of the recipient named above. We do not waive confidentiality in the event this mail was transmitted wrongly. If you have received this communication in error, and are not the intended recipient, you are hereby notified that you are prohibited from reading, printing, copying, or disseminating this message, any part of it, or any of the attachments it may carry. If you have received this message in error, please destroy all electronic and paper copies and notify the sender immediately of the inadvertent transmission. We would like to advise you that we would not waive any of our privilege for taking action against you in the event the confidentiality of this message has been compromised. Thank you for your cooperation
________________
This email has been scanned by the MessageLabs Email Security System.
For more information please visit http://www.messagelabs.com/email
______________________________________________________________________

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


THIS MESSAGE IS ONLY INTENDED FOR THE USE OF THE INTENDED RECIPIENT(S) AND MAY CONTAIN INFORMATION THAT IS PRIVILEGED, PROPRIETARY AND/OR CONFIDENTIAL. If you are not the intended recipient, you are hereby notified that any review, retransmission, dissemination, distribution, copying, conversion to hard copy or other use of this communication is strictly prohibited. If you are not the intended recipient and have received this message in error, please notify me by return e-mail and delete this message from your system. Ontario Power Generation Inc.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...