Re: [MW:7170] RE: 7151] Re: Delta ferrite Drg

Hi,
Delta Ferrite Drawing is a diagram predicting Ferrite content in Stainless steels.You can measure the ferrite content by many of the method by NDE.If you are not having such facilities you can ask NDE company to measure the Ferrite Number and the will give you the result with Delta ferrite diagram(Chromium equivalent vs nickel equivalent).you can see the sample file attached with this.
Ferrite number is a measure of Chromium & Nickel equivalent in an Austenitic stainless steel material.Normally client wants to make sure the FN in Austenitic welds which has exceed or not.
 
Thanks & Regards,
(Karthik)

On Thu, Sep 23, 2010 at 10:50 AM, PB HEGDE <hegde.pb@isgec.com> wrote:

Dear Mr Herman Pieper
Client wants specifically "Delta Ferrite Drawing" Which I could not
understand
Regards

Hegde P.B.

-----Original Message-----
From: materials-welding@googlegroups.com
[mailto:materials-welding@googlegroups.com] On Behalf Of hpi001
Sent: Wednesday, September 22, 2010 9:23 PM
To: Materials & Welding
Subject: [MW:7151] Re: Delta ferrite Drg

Dear Mr. Hedge,

I assume that they mean the delta ferrite skeleton in weld connections
of Austenitic Stainless Steels. You need a minimum of 2 - 6 % Delta
Ferrite in order to avoid hot cracks. By way of the ferrite skeleton
in the weld metal you can show that this is present (continue skeleton
instead of a under broken skeleton). I hope you understand what I
meant because I don't now exactly how to put this in English.

Best Regards,


Herman Pieper

On 22 sep, 13:19, "PB HEGDE" <hegde...@isgec.com> wrote:
> Dear friends
>
> Request to share information about " Delta ferrite Drawing " which is
asked
> by one of our client i.e. what is the meaning of Delta Ferrite Drawing ?
>
> Regards
>
> Hegde P.B.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to
materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and
meant for educational purposes only, Users must take their own decisions
w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...