material used is not A514 OR A517. material used is  of very low grade. it is welding of angle bar. also the environment will be dry.  it is structural work only used to provide addtional support to  a grout and wall. the use of E6010 is allowed for this joint. but because of the unavailaibilty of  E6010 ,  the E 7018 Electrode has been used.
 
Also i think if the electrodes  E 7018 are provided in hermetically sealed containers  baking is not required.

On Mon, Sep 27, 2010 at 7:09 AM, Karthik <karthik6684@yahoo.com> wrote:
Hi,
Please find below the comments on your quiery.
what will be the effect in Mechanical/chemical proerties of deposited weld metal of  E7018 which is used for Structural welding of angle bar( material CS) without drying  (at 260-430deg C) and Holinding(at 120 deg C).
  
Can E7018 be used without proper drying and holding for stuructural welding( fillet weld only) of angle bar/supports(material CS).
 
No.
Using of Elctrodes without baking will leads to under-bead cracking. Usually whatever code that you are welding to will detail the process. API, AWS or whatever. It's the hydrogen trapped in the weld that makes the difference. Depending upon materials, the defect may not be detectable for several days.
 
Also Pls.Find below the Extraction from AWS D1.1 for electrode restrictions on A514 and A517(if it is applicable to you)

5.3.2.5 Electrode Restrictions for ASTM A 514 or

A 517 Steels. When used for welding ASTM A 514 or

A 517 steels, electrodes of any classification lower than

E100XX-X, except for E7018M and E70XXH4R, shall

be baked at least one hour at temperatures between

700°F and 800°F [370°C and 430°C] before being used,

whether furnished in hermetically sealed containers or

otherwise.

 


 
Karthikeyan.S
QA/QC Manager
Getabec Energy Co.,Ltd.
379,Moo6,Soi8,Nikhomphatana,
Rayong-21180,
Thailand.
Phone: 0066 38 897035-8 (Off)
Fax: 0066 38 897034
Hand Phone: 0066 892512282


--- On Sun, 9/26/10, asad azmi <azmiasadayub@gmail.com> wrote:

From: asad azmi <azmiasadayub@gmail.com>
Subject: [MW:7196] use of E 7018 Electrode for stuructural welding without proper drying and holding Date: Sunday, September 26, 2010, 11:08 AM

Dear All,
 
Goodday.
 
 
what will be the effect in Mechanical/chemical proerties of deposited weld metal of  E7018 which is used for Structural welding of angle bar( material CS) without drying  (at 260-430deg C) and Holinding(at 120 deg C).
 
 
Can E7018 be used without proper drying and holding for stuructural welding( fillet weld only) of angle bar/supports(material CS).
 
 
Thanks in advance for your valuable suggestions.
 
Best  Regards
 
Asad Azmi
 
 
 
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...