Skip to main content

RE: [MW:3845] welding electrode requirement

AWS D14.1/D14.1M, Specification for Welding of Industrial and Mill Cranes and Other Material Handling Equipment will provide guidance for welding of gantry rails.  It can be purchased from the American Welding Society bookstore at www.aws.org.
 
David Landon
Vermeer Corporation


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of agmendoza@cantv.net
Sent: Tuesday, December 15, 2009 7:36 AM
To: materials-welding@googlegroups.com
Subject: Re: [MW:3841] welding electrode requirement

Hi freen

In these steel the weldability is good, but most tipes of carbon content can present problems of crack.

Preferably shall by weld with  low hodrogen electrode.

Check the carbon content and selecting the filler material.

Kind regards

Gustavo Mendoza
----------- Mensaje Original --------------

De: SLM [smahuri@lntecc.com]
Para: materials-welding@googlegroups.com [materials-welding@googlegroups.com]
Cc:
Asunto: [MW:3840] welding electrode requirement
Fecha: 15/12/2009 04:15:51
Mensaje:

Hi,

 

Kindly, let me know which welding electrode should be applied for welding of following material

 

1.       IS 1364 to IS 1030 material.

2.       Any precautions requirement for welding of above material

 

The following material is to be used for Gantry Rail

 

 

 

Regards,

 

Snehkumar L Mahuri

Region Quality Manager

M : 09909914456

 



"This Message and its contents is intended solely for the addressee and is proprietary.Information in this mail is for L&T Business Usage only. Any Use to other than the addressee is misuse and infringement to Proprietorship of L&T ECC.If you are not the addressee please return the mail to the sender.L&T ECC DIVISION"

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogs pot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...