Re: [MW:3811] Welding of P5A & P5B Material

Thank for your quick replay,

 Yes, it is there in ASME B31.1, as per 131.4.5- Preheating & as per Table 132- Post weld heat treatment.

But my question is related to post heating, means after complication of welding, immediately we have to do post heating for 2 hours @ 250˚C or 2.5 hors @ 200˚C ……( it is not a PWHT)

 

Please give me some information for this P5A & P5B material, because we have to establish new procedure for those materials……

 

Regards

K.C.Chavda

--- On Wed, 12/9/09, Devarajan Ramasamy <neo.devarajan@gmail.com> wrote:


From: Devarajan Ramasamy <neo.devarajan@gmail.com>
Subject: Re: [MW:3810] Welding of P5A & P5B Material
To: materials-welding@googlegroups.com
Date: Wednesday, December 9, 2009, 2:45 PM

Refer to ASME B31.1 page 83 and 84 for preheating and post heating requirement for P5A and P5B. Generally, the minimum thickness for preheating & post heating for P5A material is above 13mm and for P5B material is above 10mm. Heating temperature for P5B material is 740 ~ 780 deg C and for P5A material is 680 ~ 720 deg C. Heating time varies with the thickness of the material. P5B material & P5A material requires argon backing.

For the welding of SA 335 Gr. P91 (PNo-5B, Group No-2) Material………
1)      What is the Preheating Temperature?
2)      What is the Post heating Temperature & Time ?
3)      PWHT is require or not ?
4)      While welding (GTAW) Backing is require if yes, then Argon is OK ?

For the welding of SA 335 Gr. P22 (PNo-5A, Group No-1) Material………
1)      What is the Preheating Temperature?
2)      What is the Post heating Temperature & Time ?
3)      PWHT is require or not ?
4)      While welding (GTAW) Backing is require if yes, then Argon is OK ?

On Wed, Dec 9, 2009 at 3:43 PM, KC <kc.chavda07@gmail.com> wrote:
Can any body inform about the …..

For the welding of SA 335 Gr. P91 (PNo-5B, Group No-2) Material………
1)      What is the Preheating Temperature?
2)      What is the Post heating Temperature & Time ?
3)      PWHT is require or not ?
4)      While welding (GTAW) Backing is require if yes, then Argon is OK ?

For the welding of SA 335 Gr. P22 (PNo-5A, Group No-1) Material………
1)      What is the Preheating Temperature?
2)      What is the Post heating Temperature & Time ?
3)      PWHT is require or not ?
4)      While welding (GTAW) Backing is require if yes, then Argon is OK ?

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
This message originated from the Internet. Its originator may or may not be who they claim to be and the information contained in the message and any attachments may or may not be accurate.

This email transmission is intended solely for the named recipient(s). It may contain confidential and/or privileged information.If you are not the intended recipient, note that disclosing, copying or distributing it may be unlawful. Please notify the sender immediately if you have received it by mistake, and delete it from your system.
Internet communications cannot be guaranteed to be timely, secure, error or virus-free. The sender does not accept liability for any errors or omissions.

"SAVE PAPER - THINK BEFORE YOU PRINT!"

Regards,

~ DEVARAJAN RAMASAMY~
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

__________________________________________________
Do You Yahoo!?
Tired of spam? Yahoo! Mail has the best spam protection around
http://mail.yahoo.com

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...