[MW:3878] RE: 3873] Product Marking of Studs from supplier, SA 193 & SA 962.

why are you referring SA 962?, is it specified in the P.O. in my opinion SA962 is applicable only when you specify in the P.O, other wise you can refer only SA193 along with SA29/484 requirements as specified.
Since there is no alteration of mechanical properties (assuming only machining and no hot work involved), the acceptance depends on the purchaser(you) and the reliability of your supplier.
Certification can be done by producer of raw material or finished fasteners supplier.
and for the purpose of identification marking, the manufacturer is considered the organization that certifies the fastener.
you may ask for some additional checks, like
 
if I am the buyer I will choose the following options for salvage
  1. dimensional check as per the requirement (for e.g  ANSI B1.1)
  2. finish of ends, flat chamfered or round as per the agreement
  3. thread engagement at the ends
  4. manufacturer marking could be available at least for some studs even after cutting the length, is it possible to correlated this marking with original manufacturers certificate?
  5. may ask  trader to get an authorization from the original manufacturer for rest of the marking
  6. trader can recertify the lot with his own marking along with the compliance certificate to the dimensional standard.
  7. additional samples could be tested for mechanical properties from the lot, sample selection by buyer's inspector.
 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of DOKKU AJAY
Sent: Tuesday, December 22, 2009 5:54 PM
To: materials-welding@googlegroups.com
Subject: [MW:3873] Product Marking of Studs from supplier, SA 193 & SA 962.

Dear All,
 
I have an issue with respect the marking on the Stud as detailed below:
 
Issue: A trading company had provided the studs (SA 193 Gr.B7) of required sizes by cutting it from a long stud bars procured  from the studs manufacturer which caused the removal of original product marking and trade mark..
 
Statement in ASME Sec.IIA , SA 962, Clause 20.5:
 
" When product is altered in a manner which changes specified requirement (in my case it's length), it is the responsibility of the current certifying organization to ensure that the product marking is appropriately revised. This includes the removal of the name or symbol of the previous certifying organisation."
 
Present condition: The studs are supplied with only "B7" Marking and the trader had informed us that marking is done by them after cutting it to the required length. Also, trader had provided us the MTC from original manufacturer.
 
Additional Documentation asked by us: We had asked the trader to provide a certification letter stating that the studs are of xx heat no's and are from xx manufacturer (attaching original manufacturer MTC.
 
Confirmation required: With the above documentation work and product marking, studs can be accepted?
 
Thanks in advance
 
Ajay
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...