Re: [Bulk] [MW:3927] WPS & PQR clarification

Before carrying out any welding, we should ensure that the resultant welding meet the requirements of code. That's why Welding procedure (WPS) is established. WPS contains all essential & non essential varibales as per referencing code, Based on WPS the test sample is welded and actual records of all essential variables are recorded. After completion of welding, the sample will go for Testing (tensile test, bend test). After successful completion of all testing, all details (welding variables) will be recorded on a form, that is called as Procedure qualification record (PQR).
 
PQR is actual welding record. This PQR  can be used to support many WPS.
 
With only Qualified WPS, we can go ahead with welding.
 
Hope this is clear.
 
Mhaskar Aly
Kuwait.


From: Chaitanya Purohit <chaitanya_purohit@yahoo.co.in>
To: materials-welding@googlegroups.com
Sent: Wed, December 30, 2009 5:01:18 PM
Subject: Re: [Bulk] [MW:3926] WPS & PQR clarification

In simple words in construction language I can explain WPS / PQR as follows....

there will be Drawing approved for Construction = WPS prepared in initial stage
Construction process as per approved Drawing = Qualifiying PQR and Testing
As built Preparation and using the approved drawing for Proto type items = Modified WPS based on PQR data, used during welding of similar welds in future

Hope I made it clear....

Regards.
C. K. Purohit
Eng-Tech Weld1
Sr Welding Inspector


2009/12/30 mahen dran <cbemahendar@yahoo.com>
Dear Group
 
 Good day,
--------------------------------------------------------------------------------------------------------------------------------
Still I have confusion on WPS and PQR terms.
 
1. WPS to be created  first , with respect to  selection of process, electrode and current  etc.
2. PQR is developed  after WPS ,by entering the the actual variation  relevant to the WPS.
 
|Corresponding reference numbers are to be entered  in each other.
 
This is the information  from ASME IX codes.
 --------------------------------------------------------------------------------------------------------------------------
But there is a controvercial  statement  from some of our colleques, PQR to be developed first and  Supporiting PQR  reference number is to be entered in the WPS.
 
Please clarify this confusion .
 
 
mahendra
KSA

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...