Dear VJ

I could not understand the exact question. There is no contradiction in the
two para's QW 200.2/200.4 as mentioned by you. Rather, 200.2 is general
rule, while QW200.4 specifies the specific requirements of preparation of
WPS using more than one PQR (QW 200.4/a) and specific
relaxations/requirements root runs (QW 200.4/b). In any case, the essential
and supplementary essential variables (when required) are required to be
supported by PQR.

Please elaborate your question, if in doubt.

Best regards,

Prasad


VJ V
<veevee17@gmail.c
om> To
Sent by: "Materials & Welding"
materials-welding <materials-welding@googlegroups.com
@googlegroups.com >
cc

24/02/09 11:02 AM Subject
[MW:1617] WPS from 2 PQRs

Please respond to
materials-welding
@googlegroups.com

Hi everyone,

I would like to know reg Sec IX,QW 200.2(f) and QW 200.4(a)

200.2(f) states " A single WPS may cover several essential variable
changes......(eg. a single WPS may cover a thinkness range from 1.5mm
thru 32mm if PQR exist for both 1.5 to 5mm and 5mm thru 32 mm ranges)

But QW 200.4(a) states if all essential/supplementary essential
variable according to QW 451 is meeting then ......

My doubt is this: As per 200.2(f), "Base metal range" is not meeting
the requirement of QW 451.

But QW 200.4(a), states base metal thickness range, weld metal
thickness range etc shall meet QW 451.

Can anybody please clarify...

Regrds


Save a tree...please don't print this e-mail unless you really need to.

Save a tree...please don't print this e-mail unless you really need to.


--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...