Skip to main content

[MW:1666] Re: Buttering on Plate

55 mm gap should not be done with buttering.here the thickness is  23.4mm.Presume that the gap is produced for vertical welding the problem shall be solved by providing backing plate of suitable thickness say 12mm or even 16mm.UT results shall be checked for crack or other weld defects
Technical details regarding backing weld shall be availed from AWS D 1.1
 
 
Regards
R.Venkataraman

Date: Sat, 28 Feb 2009 10:56:43 +0400
Subject: [MW:1663] Buttering on Plate
From: pkhormis@gmail.com
To: materials-welding@googlegroups.com

Dear All!!!
 
We are doing some Tanks as per API 650. In one of that tank ,we faced a problem like shortened the lingth of plate..and JOINT GAP became more than the required 'Root gap'. Almost   "55mm" we got .So we thought about 'Buttering'. But in API 650 not mentioned any thing about 'buttering'. So which standard we have to follow for it, and what are the test we have to conduct over there.
 
There was no PWHT as per WPS,Pre heat was only upto 40 ^0 C.
 
plate thickness is 23.4mm- 'Double 'v' groove' , ASTM 573.GR 70.

--
PRADEEP KUMAR HORMIS




--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...