Skip to main content

[MW:1624] RE: 1623] RE: 1622] RE: 1620] PIPE SA106GRB

Dear Ravi,

 

I believe CKP has a point. This forum is not how learned you are but how you can spare learning to those who wanted to learn.

I am new to the forum and I find it so interesting and helpful. Hoping to pitch in some recommendation in the future.

 

Let’s keep an open mind guys.

 

Regards,

 

Faigal Fernando Agbanawag
Sr. Piping Engineer
Clough ZFP

T +966 3 8828818 Ext: 241
F +966 3 8828622
M +966 (0) 507780576


Disclaimer: This email and any files transmitted with it are confidential and intended solely for the use of the addressee(s) named herein. If you are not the intended recipient or addressee, you should not use, disseminate, distribute, copy or alter this email. Any views or opinions presented in this email are solely those of the author and might not represent those of "CZFP".

Warning: Although reasonable precautions have been taken to ensure no viruses are present in this email, "CZFP" cannot accept responsibility for any loss or damage arising from the use of this email or attachments. If you have received this electronic mail message in error, please contact the sender directly.

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Chaitanya Purohit
Sent: Wednesday, February 25, 2009 10:25 AM
To: materials-welding@googlegroups.com
Subject: [MW:1623] RE: 1622] RE: 1620] PIPE SA106GRB

 

Dear Ravi,

 

The intension of joining such forum is to learn more and upgrade yourself. We definitely will have such person who may ask some question like this but as a knowledgeable, mature and senior person we shall not get annoyed for such questions. Instead we shall train them to find the answers for themselves.  

 

Or else if we do not want to see such basic (may be baseless) question better define that this forum is for experts only and no junior person shall raise any question…isn’t it…

 

Don’t feel hurt about my mail but we have to put ourselves in their shoe and think like them.

 

Regards.

 

C. K. Purohit

General Manager - QC

KNM Process Systems Sdn Bhd - Malaysia

 

HP No. : 6016-3376448


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Yeleswarapu, Ravi
Sent: Wednesday, February 25, 2009 2:41 PM
To: materials-welding@googlegroups.com
Subject: [MW:1622] RE: 1620] PIPE SA106GRB

 

Suggestion,

It is a request to all members to make better use of this forum and refrain from misusing and posting such queries and wasting the valuable forum time/space without doing proper preparatory work. In my opinion cannot be answer for every ‘why’ and need not be discussed.

For following the answer is b’cos the standard states so.

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Srinivasan R.
Sent: Wednesday, February 25, 2009 10:16 AM
To: materials-welding@googlegroups.com
Subject: [MW:1620] PIPE SA106GRB

 

Why SA106GRB  pipe is available only as  seamless pipe and not welded.

 

Regards ,

 

Srinivasan.R

Piping Dept.

 

 

 

~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~
This email message is for the sole use of the intended recipient(s) and may contain confidential and privileged information of Cameron and its Operating Divisions. Any unauthorized use or disclosure is prohibited. If you are not the intended recipient, please contact the sender by reply email and delete and destroy all copies of the original message inclusive of any attachments.
~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~

 



***DISCLAIMER NOTICE ***

"This email and any files transmitted with it is confidential and is intended only for the use of the recepient(s) named above. If you are not the intended recipient, any review, retransmission, dissemination, distribution, printing, copying or use the information contained in this message or any part thereof in other manner is strictly prohibited. If you receive this email in error, please notify the sender immediately by return email and delete the email and any of its attachments. Any personal views or opinions expressed by the sender shall be understood as neither given nor endorsed by KNM or any of the companies within the Group."




 

 

 


--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...