[MW:1638] Re: WPS from 2 PQRs

Dear Prasad,
Let me make it clear...

QW 200.2(f) states about One WPS from several PQRs and vise versa.

Assume, I have got a PQR of GTAW of 4mm thick, and another PQR of 10mm
thick SMAW.
I would like to write a WPS for 20mm thick with GTAW+SMAW as the above
mentioned PQRs supporting(Assume all other variables are meeting the
req.)----Is it possibe ?

Is it possibel to write a WPS of (4+10)x 2 = 28mm thick (2t range)?

As I qouted earlier, QW 200.2(f) gives an example about write a WPS
for 1.5mm thick thru 32mm thick.So the PQRs may be of (1)which cover
upto 1.5mm to 5mm thick for its WPS (2) which cover from 5mm to 32mm
thick.

Regards


On Feb 24, 10:02 am, VJ V <veeve...@gmail.com> wrote:
> Hi everyone,
>
> I would like to know reg Sec IX,QW 200.2(f) and QW 200.4(a)
>
> 200.2(f) states " A single WPS may cover several essential variable
> changes......(eg. a single WPS may cover a thinkness range from 1.5mm
> thru 32mm if PQR exist for both 1.5 to 5mm and 5mm thru 32 mm ranges)
>
> But QW 200.4(a) states if all essential/supplementary essential
> variable according to QW 451 is meeting then ......
>
> My doubt is this: As per 200.2(f), "Base metal range" is not meeting
> the requirement of QW 451.
>
> But QW 200.4(a), states base metal thickness range, weld metal
> thickness range etc shall meet QW 451.
>
> Can anybody please clarify...
>
> Regrds

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

Comments

Popular posts from this blog

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

The Schaeffler and Delong diagrams for predicting ferrite levels in austenitic stainless steel welds

Introduction Ferrite is important in avoiding hot cracking in during cooling from welding of austenitic stainless steels. 'Constitution diagrams' are used to predict ferrite levels from the composition by comparing the effects of austenite and ferrite stabilising elements. The Schaeffler and Delong diagrams are the original methods of predicting the phase balances in austenitic stainless steel welds. Nickel and chromium equivalents A 'nickel equivalent' is calculated for the austenite stabilising elements and a 'chromium equivalent' ferrite stabilising elements. These are used as the axes for the diagrams, which show the compositional equivalent areas where the phases austenite, ferrite, martensite (and mixtures of these) should be present. Although intended to show the phase balance of weld fillers, these diagrams can also be used to illustrate the phase balance of the 'parent' material. There are different diagrams for dif...