[MW:1603] Re: 1599] Re: Pneumatic test of Reinforcement Pad for Branch connection in Piping

I don't agree with both the reply. RP wrote that it is mandatory
otherwise how we can understand the leakage? If code or client's spec
doesn't require leak test, why we have to do? Of course it is better
to do. Like better to do 100% RT, but in case of 10% requirement, we
accept balance 90% on the basis of 10%. Same way code considers that
the welding between run and branch pipes are OK. More over leaks may
be also from vent holes.
SS wrote that during hydrotest of main line, we can also find leakage
in RF pad. I think this is completely wrong, otherwise we have to
change the fitter, welder and welding inspector immediately.

Regards,
R. Bose

On Feb 19, 6:16 am, "S SIVASUBRAMANIAN" <s...@lntkuwait.com> wrote:
> Dear Mr. Jivan Dhamane,
>
> As per ASME B31.3 Pneumatic test of RF pad is not mandatory, if there is any
> defect in RF Pad weld, during hydrotest of the main line you can find out
> because of the Hydrostatic pressure in main line.
>
> With regards,
>
> S. SIVASUBRAMANIAN
>
> QA/QC Manager
>
> Larsen & Toubro Kuwait Construction Company
>
> P.O. Box.1082, Fintas 51011, KUWAIT
>
> Mobile: 00965 66387188, 00965 94005327
>
> Fax: 00965 66321511
>
>   _____  
>
> From: materials-welding@googlegroups.com
> [mailto:materials-welding@googlegroups.com] On Behalf Of Ramprasad Chari
> Sent: Thursday, February 19, 2009 6:55 AM
> To: materials-welding@googlegroups.com
> Subject: [MW:1599] Re: Pneumatic test of Reinforcement Pad for Branch
> connection in Piping
>
> Irrespective of, whether it is mentioned in code or not RF pad has to be
> pneumatically tested otherwise how will you check leakage in "welds"
> associated with RF pad.
>
> Regards
>
> Aarpee
>
> On Wed, Feb 18, 2009 at 10:07 PM, Jivan Dhamane <jivanadham...@yahoo.co.in>
> wrote:
>
> Dear Friends
>
> I would like to know whether Pneumatic Test of Reinforcement Pad for branch
> connection of Process Piping is mandatory as per ASME B31.3. I searhed but I
> could not found any paragraph in ASME B31.3.
>
> Regards
>
> Jivan Dhamane
>
>   _____  
>
> Cricket on your mind? Visit the ultimate cricket website. Enter now!
> <http://in.rd.yahoo.com/tagline_cricket_1/*http:/beta.cricket.yahoo.com>

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...

Re: [MW:10788] ON PLOT PIPING & OFF PLOT PIPING

Piping systems involved for the flow lines and gathering lines from the well head isolation valve to the production facility or processing plant isolation valve are determined as OFF PLOT. ON PLOT defines piping system in the processing plant and production platform. ANSI/ASME B31.4 applies for off plot piping system. B31.4 allows the use of either API 1104 or ASME section IX (as appropriate). However, occasionally, a very small system such as piping within 500 feet of a processing plant (some client also said 400 feet) may be declared B31.3 rather than B31.4. When B31.3 is invoked, only ASME Section IX is used. before you decide which code to use for welding procedure and/or welder qualification for pipe welding, you have to know the design and construction code applicable to the system. Please read far enough into scope and diagram illustrating the application of either B31.3 and B31.4 hope this helps rgds 2011/4/21 pradip kumar sil < pradipsil@gmail.com > Dear all, ...