Skip to main content

[MW:1600] RE: 1599] Re: Pneumatic test of Reinforcement Pad for Branch connection in Piping

Dear Mr. Jivan Dhamane,

 

As per ASME B31.3 Pneumatic test of RF pad is not mandatory, if there is any defect in RF Pad weld, during hydrotest of the main line you can find out because of the Hydrostatic pressure in main line.

 

With regards,

 

S. SIVASUBRAMANIAN

QA/QC Manager

Larsen & Toubro Kuwait Construction Company

P.O. Box.1082, Fintas 51011, KUWAIT

Mobile: 00965 66387188, 00965 94005327

Fax: 00965 66321511


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Ramprasad Chari
Sent: Thursday, February 19, 2009 6:55 AM
To: materials-welding@googlegroups.com
Subject: [MW:1599] Re: Pneumatic test of Reinforcement Pad for Branch connection in Piping

 

Irrespective of, whether it is mentioned in code or not RF pad has to be pneumatically tested otherwise how will you check leakage in "welds" associated with RF pad.

Regards

Aarpee

On Wed, Feb 18, 2009 at 10:07 PM, Jivan Dhamane <jivanadhamane@yahoo.co.in> wrote:

Dear Friends

 

I would like to know whether Pneumatic Test of Reinforcement Pad for branch connection of Process Piping is mandatory as per ASME B31.3. I searhed but I could not found any paragraph in ASME B31.3.

 

Regards

 

Jivan Dhamane

 


Cricket on your mind? Visit the ultimate cricket website. Enter now!




--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...