[MW:1659] Re: A333 Material for impact test requirement

First of all, let me clarify that A333 material is intended for low
temperature service only. So it is unlikely that the material is not impact
tested except for grade-11

ASTM A333 calls for impact testing (except grade-11) as per the material
standard itself when the thickness exceeds 3 mm. (Refer Para-8 and
Table-5).

So far as the impact testing of material (as per design standard) is
concerned, I feel it is very well explained in Para 323.2.2(particularly
sub para a) and Table 323.2.2. Other/subsequent para's are also elaborative
for the exact requirement for various materials. Also, refer the Fig.
323.2.2A for other materials.

I hope this has clarified. As a matter of fact, I could not follow your
exact question. If you have any particular doubt, pl. specify otherwise, it
seems to be a hypothetical question.

Best regards,

Prasad


"Faigal Fernando
Agbanawag"
<faigal.agbanawag To
@czfp.com> <materials-welding@googlegroups.com
Sent by: >
materials-welding cc
@googlegroups.com
Subject
[MW:1655] A333 Material for impact
26/02/09 04:06 PM test requirement


Please respond to
materials-welding
@googlegroups.com


Dear all,

Can anybody elaborate chapter III of B31.3 regarding the impact test
requirement of ASTM A333 where in section 323.2.2 states the limitation
concerning impact testing of a particular material. Is it mandatory for
A333 to have an impact test ?, where low temperature service is not an
issue.

Your response are highly appreciated.

Regards,

Faigal Fernando Agbanawag
Sr. Piping Engineer
Clough ZFP



T +966 3 8828818 Ext: 241

F +966 3 8828622

M +966 (0) 507780576


Disclaimer: This email and any files transmitted with it are confidential
and intended solely for the use of the addressee(s) named herein. If you
are not the intended recipient or addressee, you should not use,
disseminate, distribute, copy or alter this email. Any views or opinions
presented in this email are solely those of the author and might not
represent those of "CZFP".


Warning: Although reasonable precautions have been taken to ensure no
viruses are present in this email, "CZFP" cannot accept responsibility for
any loss or damage arising from the use of this email or attachments. If
you have received this electronic mail message in error, please contact the
sender directly.


Save a tree...please don't print this e-mail unless you really need to.

Save a tree...please don't print this e-mail unless you really need to.


--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...