Dear Winarko,

As per API 650, Please refer the alternative testing If sufficient water not available in the article 7.3.5 testing of shell, point no -2.

"2. If sufficient water to fill the tank is not available, the tank may be tested by (1) painting all of the joints on the inside with a
highly penetrating oil, such as automobile spring oil, and carefully examining the outside of the joints for leakage; (2)
applying vacuum to either side of the joints or applying internal air pressure as specified for the roof test in 7.3.7 and carefully
examining the joints for leakage; or (3) using any combination of the methods stipulated in 7.3.5, Subitems 1 and 2.

Regards,
Oarag.


On Friday, October 16, 2015 at 6:51:40 AM UTC+3, pras ari wrote:
Dear Prakash,

I use API 650, Is any others option for substitute leak test?

Thanks & Regards
Winarko

On Tuesday, October 13, 2015 at 8:57:45 PM UTC+8, Prakash Gotimukul wrote:
Pl refer UL 142 standard for deisel tanks

Rgds
G.Prakash
Independent Consultant, ASME/ISO/PED
Tel: +9714 2778511 Mob:+97152 979 5678

On Tue, Oct 13, 2015 at 1:57 PM, pras ari <alhani...@gmail.com> wrote:
Dear Sir,

Please advise me about leak test (hydro-test) of HSD Fuel Tank, I have 2 (two) tank with capacity 1400 KL, We will held Leak test but but site condition and around very difficult to get water as much as 2800 kilo liters.
Is any method for substitute leak test? may be NDT or pneumatic test?


Thanks & Regards
Winarko

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAMoAFwrSgBgmU-%3DZKEuaK_YigrM5eBnzrYfTHsyrm%2BUvMSuYcg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/3a32d713-a16e-43aa-8ea6-c8352f7d78ac%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

Comments

Popular posts from this blog

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...

[MW:5202] RE: 5200] NDT after PWHT

------------------------------------- Interpretation:  I‑89‑14 Subject:         Section I (1986 Edition, 1987 Addenda), PW‑11,                  NDE Prior to PWHT Date Issued:     December 15, 1988 File:            BC88‑393   Question: Does PW‑11 require that NDE be performed on welds after they have been subjected to the postweld heat treatment required by PW‑39?   Reply: No, unless the conditions described in PW‑11.2.2 exist. ---------------------------------------------- Interpretation:  VIII-1-98-09 Subject:         Section VIII, Division 1 (1995 Edition, 1996 Addenda); NDE                 ...

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...